Published: 01 June 2019
Fig. 1 Section of an RA 333 radiant tube that corroded in a heating furnace. Top: hole corroded in tube wall and locations where three metallographic specimens were removed. Bottom: specimens etched with mixed acids showing microstructure of specimen 1 at various depths in corroded region More
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.steel.c0046995
EISBN: 978-1-62708-232-7
... of the burners. The tubes had an original wall thickness of 3.0 mm (0.120 in.) and were made of three different alloys: the first was Hastelloy X; the second alloy was RA 333, a wrought nickel-base heat-resistant alloy; and the third was experimental alloy 634, which contained 72% Ni, 4% Cr, and 3.5% Si...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.steel.c0046998
EISBN: 978-1-62708-232-7
... Abstract One of 14 vertical radiant tubes (RA 333 alloy) in a heat-treating furnace failed when a hole about 5 x 12.5 cm (2 x 5 in.) corroded completely through the tube wall. The tube measured 183 cm (72 in.) in length and 8.9 cm (3 in.) in OD and had a wall thickness of about 3 mm (0.120...
Image
Published: 01 June 2019
Fig. 1 Three radiant tubes from a carburizing furnace that failed by corrosion. (a) Corroded portions of tubes made of Hastelloy X (top), experimental alloy 634 (center), and RA 333 alloy (bottom). 0.3x. (b) to (d) Unetched sections from corroded portions of the tubes: (b) alloy 634 tube More