Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0001819
EISBN: 978-1-62708-180-1
...Abstract Abstract This article commences with a description of the prosthetic devices and implants used for internal fixation. It describes the complications related to implants and provides a list of major standards for orthopedic implant materials. The article illustrates the body environment...
Series: ASM Failure Analysis Case Histories
Volume: 1
Publisher: ASM International
Published: 01 December 1992
DOI: 10.31399/asm.fach.v01.c9001133
EISBN: 978-1-62708-214-3
... did not occur during the sintering thermal cycle. It was recommended that the prosthetic manufacturer investigate atmosphere controls for all thermal cycles prior to coating. Adhesion Bonding strength Interface reactions Powder coating Surgical implants ASTM F75 UNS R30075 Surface...
Series: ASM Failure Analysis Case Histories
Volume: 2
Publisher: ASM International
Published: 01 December 1993
DOI: 10.31399/asm.fach.v02.c9001266
EISBN: 978-1-62708-215-0
.... The extremely coarse grain size was considered a major factor in strength reduction. Castings Grain size Prosthetics Surgical implants 316L Fatigue fracture Background Visual Examination of General Physical Features Testing Procedure and Results Discussion Conclusion...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001803
EISBN: 978-1-62708-241-9
... N. : “ Fracture Characteristics of Fatigued Ti6Al4V ELI as an Implant Material ,” Mater. Sci. Eng. A , 1998 , 243 , pp. 237 – 243 . 10.1016/S0921-5093(97)00807-1 28. McGee M.A. et al. : “ Implant Retrieval Studies of the Wear and Loosening of Prosthetic Joints: A Review ,” Wear...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001845
EISBN: 978-1-62708-241-9
... B. , Wang R.F. , Lang B.R. , Finite element analysis to determine implant preload . J. Prosthet. Dent . 900 ( 6 ), 539 – 546 ( 2003 ) 10.1016/j.prosdent.2003.09.012 8. Karalis D.G. , Melanitis N.E. , Pantelis D.I. , Failure analysis of a rock anchor made...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.homegoods.c9001610
EISBN: 978-1-62708-222-8
... , 1987 , pp. 547 – 65 . 12. Fraker A.C. : Corrosion of Metallic Implants and Prosthetic Devices , Corrosion , vol. 13 , Metals Handbook , 9th ed. , ASM International , 1987 , pp. 1324 – 35 . 13. Faust C.L. : Electropolishing , Heat Treating, Cleaning and Finishing , vol...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.med.c9001690
EISBN: 978-1-62708-226-6
... on the screw head In all prosthetic devices—particularly those having multicomponents—the regions of stress concentration often coincide with crevice areas where localized corrosion is more likely. 24 The presence of surface irregularities locally increases the stress concentration, and dramatically...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003539
EISBN: 978-1-62708-180-1
... Used for Prosthetic Devices,” Ph.D. dissertation, UCLA , 1977 24. Lund R.A. and Fowler G.J. , Intergranular Fracture in Engineering Materials , International Symposium for Testing and Failure Analysis , ISTFA, 1984 , p 311 – 321 25. Liaw P.K. , Leax T.R...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006776
EISBN: 978-1-62708-295-2
... Casting Alloy Used for Prosthetic Devices ,” Ph.D. dissertation, UCLA , 1977 26. Lund R.A. and Fowler G.J. , Intergranular Fracture in Engineering Materials , International Symposium for Testing and Failure Analysis (ISTFA) , 1984 , p 311 – 321 27. Liaw P.K. , Leax...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006811
EISBN: 978-1-62708-329-4
.... J. , Vol 25 , 1998 , p 282 – 293 49. Pibarot P. and Dumesnil J.G. , Prosthetic Heart Valves Selection of the Optimal Prosthesis and Long-Term Management , Circulation , Vol 119 , 2009 , p 1034 – 1048 10.1161/CIRCULATIONAHA.108.778886 50. Matchett M. , Sears...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006813
EISBN: 978-1-62708-329-4
...(03)00062-1 19. Al Jabbari Y.S. , Fournelle R. , Ziebert G. , Toth J. , and Iacopino A.M. , Mechanical Behavior and Failure Analysis of Prosthetic Retaining Screws after Long-Term Use In Vivo, Part 4: Failure Analysis of 10 Fractured Retaining Screws Retrieved from...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.9781627083294
EISBN: 978-1-62708-329-4