...Abstract Abstract A failure analysis was conducted on a flow-sensing device that had cracked while in service. The polysulfone sensor body cracked radially, adjacent to a molded-in steel insert. This article describes the investigative methods used to conduct the failure analysis...
Book Chapter

Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003541
EISBN: 978-1-62708-180-1
... of solvents. When an active solvent causes the crazing stress to fall below the shear yielding stress, a polymer that normally exhibits ductile failures under tensile loading can show brittle failures precipitated by the crazing. Such solvent effects can be observed in failures of PC and polysulfone ( Ref 7...