1-2 of 2 Search Results for

Polyacetal

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.homegoods.c0090457
EISBN: 978-1-62708-222-8
... to secure a metal slide on an older design, whereas newer components showed no signs of failure. The latch assembly components were injection molded from an unfilled commercial grade of a polyacetal copolymer. Investigation of failed parts (including visual inspection, a specially designed proof load test...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003525
EISBN: 978-1-62708-180-1
... Example 11: Cracking of a Polyethylene Chemical Storage Vessel Example 12: Failure of Polyacetal Latch Assemblies Example 13: Failure of a Nylon Filtration Unit Example 14: Failure of a PC Switch Housing Example 15: Failure of Nylon Hinges Tests and Results Conclusions Tests...