Published: 15 May 2022
Fig. 4 X-ray image showing displaced wires in an electrofusion pipe fitting connection. Courtesy of Element New Berlin More
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.modes.c9001699
EISBN: 978-1-62708-234-1
... a recirculating capacity of about 44,000 gal (166,000 L) of water. It consisted primarily of steel pipes fitted with threaded connectors on the 2 in. (46 cm) pipes and bolted flanged couplings on the larger pipes. Seven years following the completion of the mall, corrosion problems were noted at the outer...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.conag.c0047570
EISBN: 978-1-62708-221-1
... section of the pipe. The toe of the weld and the adjacent undercut were stress raisers that determined the point of major crack origin. Under residual stress, the internal point of incomplete fusion also initiated additional cracks. Recommendations included ensuring a proper fit between an elliptical...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.petrol.c0048698
EISBN: 978-1-62708-228-0
.... The tee joint in the piping between the heat exchanger and the sieve bed failed after 12 months. A hole in the tee fitting and a corrosion product on the inner surface of the pitting was revealed by visual examination. Iron sulfide was revealed by chemical analysis of the scale which indicated hydrogen...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.power.c0048747
EISBN: 978-1-62708-229-7
... contributed to the failure. Recommendations included changing the joint design to incorporate a large-radius corner and improving fitting of the components to permit full weld penetration. Backing strips were suggested to increase weld quality, and the pipe wall thickness was increased from 8 to 9.5 mm...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.process.c0089734
EISBN: 978-1-62708-235-8
.... Fillet welds Flanges Headers Pipe fitting Stress concentration Superheaters Thermal stresses Weld defects ASTM A106 grade B UNS K03006 ASTM A105 grade 2 Fatigue fracture Joining-related failures A system of carbon steel headers, handling superheated water of 188 °C (370 °F) at 2 MPa (300...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.modes.c0048361
EISBN: 978-1-62708-234-1
... Abstract Several failures occurred in 64-mm schedule 80 type 304 stainless steel (ASME SA-312, grade TP304) piping in a steam-plant heat-exchanger system near tee fittings at which cool water returning from the heat exchanger was combined with hot water from a bypass. Various portions...
Series: ASM Failure Analysis Case Histories
Volume: 1
Publisher: ASM International
Published: 01 December 1992
DOI: 10.31399/asm.fach.v01.c9001057
EISBN: 978-1-62708-214-3
... and background evidence obtained indicated failure due to cracking initiated by stamped markings on the pipe wall and extended by high circumferential residual stresses. It was recommended that annealed pipe be used. Cracking (fracturing) Pipe fittings Plumbing Transgranular fracture 230 UNS C23000...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.power.c0047621
EISBN: 978-1-62708-229-7
..., and flange and more skillful welding techniques to avoid undercutting and unfused interfaces. Arc welding Combustion chamber Flanges Gas turbine engines Pipe fitting Undercuts Welding defects Inconel 718 (Nickel-base superalloy) UNS N07718 Fatigue fracture Joining-related failures...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.modes.c0046991
EISBN: 978-1-62708-234-1
... Abstract The outlet-piping system of a steam-reformer unit failed by extensive cracking at four weld locations. The welded system consisted of Incoloy 800 (Fe-32Ni-21Cr-0.05C) pipe and fittings. The exterior surfaces of the system were insulated with rock wool that did not contain...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.modes.c0048846
EISBN: 978-1-62708-234-1
... Abstract A main steam pipe was found to be leaking due to a large circumferential crack in a pipe-to-fitting weld in one of two steam leads between the superheater outlet nozzles and the turbine stop valves (a line made of SA335-P22 material). The main crack surface was found to be rough...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.bldgs.c9001701
EISBN: 978-1-62708-219-8
.... The fittings were mechanically threaded assemblies. Temperatures ranged from 150 to 155 deg F (65.6 to 68.3 deg C). Leaks in the system had reportedly initiated immediately after the building had been placed in service. The cause of corrosion inside the steel pipes was attributed to tuberculation caused...
Series: ASM Failure Analysis Case Histories
Volume: 2
Publisher: ASM International
Published: 01 December 1993
DOI: 10.31399/asm.fach.v02.c9001282
EISBN: 978-1-62708-215-0
... baths, environment Nuclear reactor components Passivation Pickling Pipe fittings Sodium-cooled reactors 316 UNS S31600 Intergranular corrosion Surface treatment related failures Pitting corrosion Background Two stainless steel components fabricated from AISI type 316 stainless steel...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.modes.c0091402
EISBN: 978-1-62708-234-1
... for ferritizing malleable iron. This resulted in lower resistance to erosion and corrosion than pearlitic malleable iron. Recommendations included replacing the elbows with heat-treated fittings with a pearlitic malleable microstructure. Impingement erosion Pearlite Pipe bends ASTM A47 grade 35018 UNS...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.chem.c9001458
EISBN: 978-1-62708-220-4
... of the basket. During spinning, the crystals were washed by town's water from a single outlet pipe fitted at one side of the centre of the basket and sterilised by steam from a multi-outlet pipe fitted at the other side. The liquid, which was forced through the filter cloth, was collected on the inside...
Series: ASM Failure Analysis Case Histories
Volume: 2
Publisher: ASM International
Published: 01 December 1993
DOI: 10.31399/asm.fach.v02.c9001327
EISBN: 978-1-62708-215-0
.... Nuclear reactor components Pipe fittings Weldments ASME SA106-B Corrosion fatigue Background During a refueling outage at a pressurized water reactor (PWR), feedwater reducers to all four steam generators were replaced. Three of the four piping reducers showed indications of flaws when...
Series: ASM Failure Analysis Case Histories
Volume: 2
Publisher: ASM International
Published: 01 December 1993
DOI: 10.31399/asm.fach.v02.c9001325
EISBN: 978-1-62708-215-0
... in the system had suffered failure. Pertinent Specifications The cross-tee was created by welding two 2-inch pipes [1] 180° apart to a run of 3-in. pipe. One 2-in. leg was welded directly to the 3-in. pipe, while the other was joined through a reduction socket fitting. The design of the cross-tee...
Image
Published: 01 January 2002
Fig. 3 Low-carbon steel tee fitting in a line leading to a natural-gas dryer that failed from hydrogen sulfide corrosion. (a) Arrangement of piping showing point of leakage in the tee fitting. (b) Inner surface of the tee fitting showing corrosion deposit and area of complete penetration More
Image
Published: 30 August 2021
Fig. 3 Low-carbon steel tee fitting in a line leading to a natural-gas dryer that failed from hydrogen sulfide corrosion. (a) Arrangement of piping showing point of leakage in the tee fitting. (b) Inner surface of the tee fitting showing corrosion deposit and area of complete penetration More
Image
Published: 01 June 2019
Fig. 1 Low-carbon steel tee fitting in a line leading to a natural-gas dryer that failed from hydrogen sulfide corrosion. (a) Arrangement of piping showing point of leakage in the tee fitting. (b) Inner surface of the tee fitting showing corrosion deposit and area of complete penetration More