Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.design.c0090436
EISBN: 978-1-62708-233-4
... resin used to produce the discrepant parts revealed that the pellets were of two general types, neither of which matched the pellets from a retained resin lot. Investigation included visual inspection, micro-FTIR in the ATR mode, and analysis using DSC. The thermograms supported the conclusion...
Series: ASM Failure Analysis Case Histories
Volume: 1
Publisher: ASM International
Published: 01 December 1992
DOI: 10.31399/asm.fach.v01.c9001109
EISBN: 978-1-62708-214-3
...Abstract Abstract Grate bars in the traveling grate indurators in several taconite processing units suffered excessive corrosion following a conversion from acid to fluxed pellet production procedures. The campaign life of the HH grade cast stainless steel bars was reduced from more than 7...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001769
EISBN: 978-1-62708-241-9
... was carried out employing Himedia biochemical test kit (Mumbai) according to the manufacturer’s instructions. 16s rRNA Gene Sequencing and Phylogenetic Analysis The cultures were grown overnight in B4M broth at 37 °C. The cultures were centrifuged at 5000×g for 15 min. The bacterial pellets were used...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.homegoods.c0092135
EISBN: 978-1-62708-222-8
... variations had reduced the safety factor to about 1.3 for lead-shot ammunition. Previous tests had also shown that lead shot was deformed extensively by impact with the bore in the choke zone of this type of gun barrel. The major stresses in the choke zone are produced by impact of shot pellets against...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003525
EISBN: 978-1-62708-180-1
..., exhibiting an endothermic transition characteristic of the melting of a nylon 6/6 resin. The results also showed a second melting transition attributed to a hydrocarbon-based impact modifier. Fig. 20 The DSC thermogram representing a molding resin pellet that had produced brittle parts...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.bldgs.c9001528
EISBN: 978-1-62708-219-8
...). The black foam insulation and the reddish brown debris from the tank OD were analyzed by Fourier transform infrared (FTIR) methods per ASTM E 1252-98 using the KBr pellet technique. However, a computer-aided comparison with over 7200 library spectra provided no definitive match with the FTIR spectrum...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.steel.c9001714
EISBN: 978-1-62708-232-7
... gas heater) that heats the reductor gas from atmospheric temperature to process temperature of 925°C and the reactor that reduces oxygen contained in the iron pellets and changes it to iron sponge at process temperature. The plant can make 1.000.000 tons of iron sponge per year. Reductor gases...
Series: ASM Failure Analysis Case Histories
Volume: 2
Publisher: ASM International
Published: 01 December 1993
DOI: 10.31399/asm.fach.v02.c9001391
EISBN: 978-1-62708-215-0
... of rupture at the top of the termination. Fig. 9 Delaminated termination on a group 6 sample, showing Valox (the pellet encapsulant) intruding on the cermet/polymer thick-film metallization interface. Metallization forced the expansion of the termination, rupturing the nickel barrier and giving...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006789
EISBN: 978-1-62708-295-2
... droplet can be almost like a metal pellet when it impacts a metal surface. Solid-particle erosion occurs in fans and any rotating device that operates in a particle-laden environment. Sand blasting to alter surface texture or remove paint is solid-particle erosion. Cavitation erosion...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003573
EISBN: 978-1-62708-180-1
... to Meet Specifications Faulty Heat Treatment Conclusions Recommendations Investigation Analysis The major stresses in the choke zone are produced by impact of shot pellets against the bore. When lead shot is used, the lead absorbs a considerable amount of the impact energy...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006797
EISBN: 978-1-62708-295-2
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003522
EISBN: 978-1-62708-180-1
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006757
EISBN: 978-1-62708-295-2
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003524
EISBN: 978-1-62708-180-1
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006787
EISBN: 978-1-62708-295-2