1-20 of 282 Search Results for

Nickel steel

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.chem.c9001172
EISBN: 978-1-62708-220-4
... Abstract Unalloyed steels and the pure nickel steels frequently used in the past can sustain significant damage from hydrogen attack in ammoniacal environments. The attack causes decarburization that leads to a loosening of the structure due to the precipitation of methane along grain...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.aero.c0048257
EISBN: 978-1-62708-217-4
... Abstract Evidence of destructive pitting on the gear teeth (AMS 6263 steel) in the area of the pitchline was exhibited by an idler gear for the generator drive of an aircraft engine following test-stand engine testing. The case hardness was investigated to be lower than specified and it was...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.power.c9001484
EISBN: 978-1-62708-229-7
... is shown in Figure 5 , this being characteristic of a 3 1 2 % nickel steel in the hardened and tempered condition. Some banding was evident, due to the persistence of the dendritic structure of the ingot from which the wheel was made, and this was also evident on a macroscopic scale on the...
Series: ASM Failure Analysis Case Histories
Volume: 2
Publisher: ASM International
Published: 01 December 1993
DOI: 10.31399/asm.fach.v02.c9001369
EISBN: 978-1-62708-215-0
... Abstract A crane long-travel worm drive shaft was found to be chipped during unpacking after delivery. Chemical analysis showed that the steel (EN36A with a case depth of 1 mm, or 0.04 inch did not meet specifications. Magnetic particle inspection revealed a crack on the side of the shaft...
Series: ASM Failure Analysis Case Histories
Volume: 1
Publisher: ASM International
Published: 01 December 1992
DOI: 10.31399/asm.fach.v01.c9001115
EISBN: 978-1-62708-214-3
.... Chemical analysis of the base metal and corrosion deposits did not detect iron or nickel sulfides, however Replacement of the remaining pipe strings according to a scheduled program was recommended. Because 9% Ni steel was not available, 13% Cr martensitic stainless steel was recommended as a replacement...
Series: ASM Failure Analysis Case Histories
Volume: 1
Publisher: ASM International
Published: 01 December 1992
DOI: 10.31399/asm.fach.v01.c9001062
EISBN: 978-1-62708-214-3
..., alloying additive Nickel steel - 9Ni Nickel steels Segregations 9 steel Intergranular fracture Casting-related failures The 9% Ni steels have been widely used for cryogenic applications, as in storage vessels and related components for liquid natural gas. Castings of 9% Ni steel...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.modes.c9001163
EISBN: 978-1-62708-234-1
... latter causes flake-like spalling. Measures to prevent SCC include stress reduction, use of austenitic steels or nickel alloys not susceptible to grain boundary attack, use of ferritic chromium steels, surface slag removal, control of temperature and chloride concentration, and cathodic protection...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.chem.c9001160
EISBN: 978-1-62708-220-4
... Abstract A corrosion resistant chromium nickel steel (X 2 Cr-Ni-Mo 18 10) worm drive used in a chemical plant at 80 deg C and 100 to 200 atm pressure to transport media containing chloride failed during normal operation. Visual inspections showed that the entire surface of the gear was covered...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.modes.c9001177
EISBN: 978-1-62708-234-1
... austenite, and therefore with increasing nickel content. Austenitic chromium-manganese steels and ferritic chromium steels are considerably more resistant. As a rule, however, these steels are unsuitable as replacement because of their greater sensitivity to pitting. Specifically effective corrosive media...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.aero.c9001717
EISBN: 978-1-62708-217-4
.... Material: 18% Nickel Maraging Steel per contractor specification, 2,068 Mpa (300,000 psi) Grade Strength: 1,931 Mpa (280,000 psi) UTS required per contractor specification 1,896 Mpa (275,000 psi) UTS required per contractor engineering drawing Treatment: Annealed at 816°C (1500°F) for 1 hour per...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001839
EISBN: 978-1-62708-241-9
... sources of hydrogen are considered as are remedial measures for controlling hydrogen content in steels. steel coils delayed hydrogen cracking austenitic stainless steel grain facets stepwise microcracking inert gas fusion analysis stacking fault energy 0.1%C-14.7%Cr-9.3%Mo-0.2%Si (low nickel...
Series: ASM Failure Analysis Case Histories
Volume: 2
Publisher: ASM International
Published: 01 December 1993
DOI: 10.31399/asm.fach.v02.c9001387
EISBN: 978-1-62708-215-0
... Abstract Nickel anodes failed in several electrolysis cells in a heavy-water upgrading plant. Dismantling of a cell revealed gouging and the presence of loosely attached black porous masses on the anode. The carbon steel top, plate was severely corroded. An appreciable quantity of black powder...
Series: ASM Failure Analysis Case Histories
Volume: 2
Publisher: ASM International
Published: 01 December 1993
DOI: 10.31399/asm.fach.v02.c9001311
EISBN: 978-1-62708-215-0
... change to type 304 stainless steel tubing made without dendritic weld seams was recommended. Heat-affected zone Nitric acid, environment Papermaking Welded joints, corrosion Inconel 600 UNS N06600 Uniform corrosion Galvanic corrosion Several nickel-base superalloy (UNS...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.design.c9001223
EISBN: 978-1-62708-233-4
... Abstract The corner of a welded sheet construction made from austenitic corrosion-resistant chromium-nickel steel showed corrosive attack of the outer sheet. This attack was most severe at the points subjected to the greatest heat during welding. Particularly large amounts of weld metal had...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.marine.c9001617
EISBN: 978-1-62708-227-3
... corrosion resistance in seawater include nickel-base alloys, for example, IN-718, IN-625, and the higher-grade stainless steels, such as SMO 254. Comparison of stress-number of cycles data for these materials and NAB shows that stainless steels appear to have a fatigue limit (at least in air) unlike the...
Series: ASM Failure Analysis Case Histories
Volume: 1
Publisher: ASM International
Published: 01 December 1992
DOI: 10.31399/asm.fach.v01.c9001126
EISBN: 978-1-62708-214-3
... oxide and covered on the back surfaces with an adherent black polyethylene plastic. Macro fractography, SEM fractography, EDX analysis, and photo elasticimetry were conducted on four of the shattered panels. Small nickel sulfide inclusions were found at the failure origins. Failure of the panels was...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001852
EISBN: 978-1-62708-241-9
... nickel surface on top of a fiberglass and epoxy plating mandrel in an electroplating bath. The mandrel is developed from an industry’s approved design from CAD files. For nickel tools of various applications, the plating might be 2 to 6 mm thick and free standing or mounted on a steel frame [ 1...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001758
EISBN: 978-1-62708-241-9
... at carbides and other microconstituents, especially in single crystal castings that do not possess grain boundaries. gas turbine engine components creep deformation overheating nickel-base superalloy interdendritic stress-rupture fracture stress-rupture testing stress-rupture life Cast...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003566
EISBN: 978-1-62708-180-1
... the same steel but with a hardness of 45 HRC are shown in Fig. 22 . The metallographic samples were nickel plated for good edge retention. Targets (see Fig. 6 ) of these hardnesses were selected because multiple impacts were required to produce spalling. A given target was struck in one location...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.mech.c0048120
EISBN: 978-1-62708-225-9
... Abstract The pawl spring which was part of a selector switch used in telephone equipment failed. The springs were blanked from 0.4 mm (0.014 in.) thick tempered 1095 steel and then nickel plated. Numerous pits around the rivet holes were revealed by microscopic examination of longitudinal...