1-13 of 13 Search Results for

Nb-106

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.process.c0045918
EISBN: 978-1-62708-235-8
...Abstract Abstract Cracks, with no other damage, were observed in a niobium alloy (Nb-106) part when it was pulled from several months of protective storage for assembly into a rocket nozzle. SEM views showed the cracks to be intergranular, with contaminant particles on a large number...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.homegoods.c9001610
EISBN: 978-1-62708-222-8
... variable of the material that may promote adverse reactions. Body piercing ISO 5832-1 Fe-17Cr-8Ni Fe-16Cr-8Ni-2.3Mo Fe-17Cr-10Ni-2.4Mo 100% Nb Pitting corrosion (Other, miscellaneous, or unspecified) failure Surface treatment related failures The body piercing of the upper portions...
Book Chapter

Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003562
EISBN: 978-1-62708-180-1
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006837
EISBN: 978-1-62708-329-4
... E415 Chemical composition, wt% C Mn P S Si Ni Cr Mo V Cu Al Ti Nb AAR M-107/M-208 class C    Maximum 0.77 0.90 0.030 0.040 1.00 0.25 0.25 0.10 0.040 0.35 0.060 0.03 0.05    Minimum 0.67 0.60 … 0.005 0.15...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.power.c9001594
EISBN: 978-1-62708-229-7
... Station. 4. CPSES Welding Manual , Procedure WLD-106, Section 6.9.1, Comanche Peak Steam Electric Station. 5. ASME Boiler And Pressure Vessel Code , Section III, Division 1, Subsections NB-/NC-/ND-, Article 4427, American Society of Mechanical Engineers , New York, NY . 6. ASME Boiler...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003536
EISBN: 978-1-62708-180-1
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003552
EISBN: 978-1-62708-180-1
... streams at pressures as high as 21 MPa (3 ksi) and temperatures up to 540 °C (1000 °F). Fig. 9 Section of ASTM A 106 carbon steel pipe with wall severely damaged by hydrogen attack. The pipe failed after 15 months of service in hydrogen-rich gas at 34.5 MPa (5000 psig) and 320 °C (610 °F...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006787
EISBN: 978-1-62708-295-2
Book Chapter

Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003548
EISBN: 978-1-62708-180-1
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.9781627083294
EISBN: 978-1-62708-329-4
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006812
EISBN: 978-1-62708-329-4
... 653—Tank Inspection, Repair, Alteration, and Reconstruction API Standard (STD) 579-1/ASME FFS-1—Fitness-for-Service API Recommended Practice (RP) 580—Risk-Based Inspection ANSI/NB-23—National Board Inspection Code API 510—Pressure Vessel Inspection Code: Maintenance Inspection, Rating...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006783
EISBN: 978-1-62708-295-2
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006834
EISBN: 978-1-62708-329-4