Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.mech.c9001596
EISBN: 978-1-62708-225-9
... the fatigue life. Based on an understanding of the compressor motion, a Monte Carlo model was developed based on a linear damage theory to predict the fatigue life of the springs during start/stop conditions. The results of this model were compared to actual test data. The model showed that the design...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003514
EISBN: 978-1-62708-180-1
... element. Examples of the use of probabilistic analysis are presented. The article concludes with an overview of some of the commercially available software programs for performing probabilistic analysis. advanced mean value method failure model first-second-order reliability methods Monte Carlo...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006803
EISBN: 978-1-62708-329-4
... of the Monte Carlo simulation method and work performed at the Los Alamos National Laboratories at the end of World War II ( Ref 12 ). The limitation of the original method is the large sample size required for convergence, which can become a problem when the individual “deterministic” model evaluation...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.aero.c0090030
EISBN: 978-1-62708-217-4
... simulation, and probabilistic analysis to assess the probability of rotor fracture. It computes the probability of fracture as a function of flight cycles, considering random defect occurrence and location, random inspection schedules, and several other random variables using either Monte Carlo sampling...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003512
EISBN: 978-1-62708-180-1
... programs, enhanced analytical modeling and prediction techniques, accurate life assessment methods, and a fortified commitment to avoid the recurrence of these failures through improved designs. The examples cited in Table 1 were serious and often tragic failures that had a great impact on structural...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006802
EISBN: 978-1-62708-329-4
..., material development, and material processing and controls and have redefined the criteria for failure. Furthermore, the pursuit of understanding how and why these failures occurred has resulted in the development of structural-integrity programs, enhanced analytical modeling and prediction techniques...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006936
EISBN: 978-1-62708-395-9
... combinations of beam steering and focal lengths and capturing all waveforms. Every reflector within that volume is interrogated from multiple angles with optimum focus. The information is combined and used to model the volume being inspected. The accuracy of this method and the resulting inspection data...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006767
EISBN: 978-1-62708-295-2
... normal stress reaches the yield strength of the material. Tresca’s theory states that yield at a point begins when the maximum shear stress equals the shear stress in a tension specimen when it begins to yield. Another common failure model is the von Mises criterion, which is based on a determination...