EISBN: 978-1-62708-214-3
..., and Inco alloy C-276) were placed directly in the hot gas stream, containing HCl and Cl2, for in situ testing. Results of this investigation showed that nickel-chromium corrosion-resistant alloys, such as Inconel 600, Inconel 625, and Inco alloy C-276, performed well in this environment. Laboratory testing...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.modes.c0047010
EISBN: 978-1-62708-234-1
.... The alloys fall in this order of decreasing strengths: Udimet 630, Inconel 718, Rene 41, H19 tool steel, British I steel, 4337V gun steel, and maraging steel. When cycled between room temperature and 540 to 650 deg C (1000 to 1200 deg F), only Udimet 630, Inconel 718, and Rene 41 retained yield strengths...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.power.c0046252
EISBN: 978-1-62708-229-7
... with air at 276 to 310 kPa (40 to 45 psi) and subjected to temperatures of 620 to 650 °C (1150 to 1200 °F) for an approximate total exposure time of 100 h at temperature. Closed-cycle operation with high-purity nitrogen gas started approximately 13 months after the piping was installed, then failed after...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.modes.c9001632
EISBN: 978-1-62708-234-1
... temperature cycles calculated to be from 400 to 30 deg C (752 to 86 deg F). The window was activated to >200 Sv/h. It was determined through analysis using remote handling techniques and hot cells that the crack initiated near a spot weld used to affix thermocouples to the window surface. In addition...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006838
EISBN: 978-1-62708-329-4
... 20 , 2018 , p 1700842 , 10.1002/adem.201700842 29. Sochalski-Kolbus L.M. , Payzant E.A. , Cornwell P.A. , Watkins T.R. , Babu S.S. , Dehoff R.R. , Lorenz M. , Ovchinnikova O. , and Duty C. , Comparison of Residual Stresses in Inconel 718 Simple...
Book Chapter

Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003548
EISBN: 978-1-62708-180-1
... environments, the cast structure of a nickel weld may be anodic to the wrought parent metals. The combination of their passive surface with their inherent resistance places nickel-chromium alloys such as Inconel alloy 600 and Hastelloy alloy C-276 in more noble positions in the traditional galvanic series...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006783
EISBN: 978-1-62708-295-2
... environments, the cast structure of a nickel weld may be anodic to the wrought parent metals. The combination of their passive surface with their inherent resistance places nickel-chromium alloys such as Inconel alloy 600 and Hastelloy alloy C-276 in more noble positions in the traditional galvanic series...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0001818
EISBN: 978-1-62708-180-1
... be made when care is not taken to ascertain that the alloy used complies with the alloy specified. In one case, several low-carbon steel nipples were inadvertently used in place of 5Cr-0.5Mo steel nipples in a pipeline containing hydrogen at 400 °C (750 °F). Failure occurred after approximately 4...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006787
EISBN: 978-1-62708-295-2
... designation Maximum temperature Ref °C °F Carbon and alloy steels AISI 1010 carbon steel 480 895 3 SA-178, grade A 510 (a) 950 (a) 4 SA-192; SA-210, grade A 510 (a) 950 (b) 4 SA-209, grade T-1A 525 (b) 975 (b) 4 1Cr-Mo-Si; SA-213, grade T-11 565...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003553
EISBN: 978-1-62708-180-1
... chloride environment at 95 °C (200 °F). Cracks are branching and transgranular. (b) Caustic SCC in the HAZ of a type 316L stainless steel NaOH reactor vessel. Cracks are branching and intergranular. There are exceptions to the general rule that stress-corrosion cracks are branched. For example, some...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006785
EISBN: 978-1-62708-295-2
... chloride solutions Zirconium alloys Aqueous chloride solutions, organic liquids, I 2 at 350 °C (660 °F) This list is not exhaustive. As metals continue to be used in more extreme environments, discovery of new metal-environment combinations that produce SCC will continue. Indeed, many metals...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.9781627083294
EISBN: 978-1-62708-329-4