... contribute directly to the formation of calcium carbonate, a critical factor in the buildup of scale and pitting corrosion on heat exchanger tubes. heat exchanger tubes pitting corrosion scale formation IA/PA mild steel scale deposits chemical analysis calcium concentration Mild steel (alloy...