1-10 of 10 Search Results for

Hydrofoils

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.marine.c0047917
EISBN: 978-1-62708-227-3
... Abstract The support bearing of a hydrofoil vessel failed after only 220 h of operation. The bearing consisted of an outer ring made of chromium-plated AISI type 416 stainless steel and an inner ring with a spherical outer surface made of AISI type 440C stainless steel, with a plastic material...
Image
Published: 01 January 2002
Fig. 8 Plastic-lined stainless steel spherical bearing for a hydrofoil that failed by corrosion fatigue. (a) Construction of bearing and location of fractures. Dimensions given in inches. (b) Fracture surface showing multiple fatigue origins (arrows) at edge of bore and on the spherical More
Image
Published: 01 June 2019
Fig. 1 Plastic-lined stainless steel spherical bearing for a hydrofoil that failed by corrosion fatigue. (a) Construction of bearing and location of fractures. Dimensions given in inches. (b) Fracture surface showing multiple fatigue origins (arrows) at edge of bore and on the spherical More
Image
Published: 30 August 2021
Fig. 15 Plastic-lined stainless steel spherical bearing for a hydrofoil that failed by corrosion fatigue. (a) Construction of bearing and location of fractures. Dimensions given in inches. (b) Fracture surface showing multiple fatigue origins (arrows) at edge of bore and on the spherical More
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.marine.c0091394
EISBN: 978-1-62708-227-3
.... The original author had failure analysis experience with a similar, seawater-filled fire main piping system in a high-performance hydrofoil ship, two decades earlier. Investigation The following design and parameters were revealed in investigation of the failure: Piping Material: Type 316/316L...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0001809
EISBN: 978-1-62708-180-1
... Under some conditions of corrosion, a material that would not fail without the corrosion can fail by fatigue. Example 2: Corrosion-Fatigue Failure of a Bearing in a Marine Environment A support bearing of a hydrofoil vessel failed after only 220 h of operation. The bearing ( Fig. 8 ) consisted...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006806
EISBN: 978-1-62708-329-4
... Fatigue Under some conditions of corrosion, a material that would not fail without the corrosion can fail by fatigue. For example, Fig. 15 shows a support bearing of a hydrofoil vessel that failed after only 220 h of operation. The bearing consisted of an outer ring made of chromium-plated AISI...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003570
EISBN: 978-1-62708-180-1
..., ship propellers and hydrofoils, mechanical devices with restricted fluid passages (e.g., seals and bearings), heat-exchanger tubes, and hydraulic structures such as spillways, gates, and tunnels that are associated with dams. Consequently, cavitation erosion is still a very active research topic...
Book Chapter

Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003548
EISBN: 978-1-62708-180-1
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006783
EISBN: 978-1-62708-295-2