Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.matlhand.c9001244
EISBN: 978-1-62708-224-2
...Abstract Abstract The cross bars of conveyor belt links that served to transport glass containers through a stress relief furnace fractured in many cases. They consisted of wires of 5 mm diam made of low-carbon Siemens-Martin steel, while the interwoven longitudinal bars were made of strip...
Series: ASM Failure Analysis Case Histories
Volume: 1
Publisher: ASM International
Published: 01 December 1992
DOI: 10.31399/asm.fach.v01.c9001104
EISBN: 978-1-62708-214-3
... belt and an unused section of new wire showed that the fracture resulted from sulfur attack and overheating during service. It was recommended that the sinter belt material be changed to Nicrofer 3220-H (alloy 800H). Belt conveyors Carburization (corrosion) Furnace conveyors Sintering furnaces...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.design.c9001578
EISBN: 978-1-62708-233-4
... Strip Caused by an Induction Furnace in a Steel Mill Case #3: Vibration of Microscope in Hospital Microsurgery Room Case #4: Torsional Vibration on a Reciprocating Pump Case #5: Ghosts Case #6: Vibration of Nuclear Magnetic Resonance Machine Case #7: Vibration Induced by Sound Case #8...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001778
EISBN: 978-1-62708-241-9
...Abstract Abstract A locked coil track rope (LCTR) is essentially composed of wires (round and rail-shaped) laid helically in different layers. These wire ropes are sometimes used in conveyors carrying empty and loaded buckets in mining areas. During service, such wire ropes may fail prematurely...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003509
EISBN: 978-1-62708-180-1
...-known example is the brittle failure of several World War II ships, which split in half while still at dockside ( Fig. 1 , Ref 2 ). The fractures originated at weld discontinuities and propagated through carbon-steel plate, which had coarse pearlite formed by furnace cooling. The existence of a coarse...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006808
EISBN: 978-1-62708-329-4
.... 47 Low-alloy steel conveyor pipe that cracked at fillet weld securing a carbon steel flange because of poor fit-up. Dimensions given in inches Fig. 48 Preferential corrosion of the vermicular ferrite phase in austenitic stainless steel weld metal. Discrete ferrite pools that are intact...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003553
EISBN: 978-1-62708-180-1
... or solution treating Failure to provide required temperature uniformity in furnaces Use of quenching practices too severe for a specific alloy or part shape Undue delay in transferring workpieces from the quenchant to the tempering furnace Many different types of surface-finishing treatments...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006785
EISBN: 978-1-62708-295-2