... by the presence of cracklike indications in machined bore surface of the annealed part. End frames Forgings Residual stress Fe-0.34C-1Cr-1.9Mn-1Si Hydrogen damage and embrittlement A number of machined end frame steel forgings made of Cr-Si-Mn alloy were showing tiny cracks during magnetic particle...