... breakage of the axle had occurred intergranularly in a brittle manner, possibly, initiated by a shallow zone of fatigue along the sharp radius acting as stress riser. Aircraft components Axles Landing gear Radii Fe-0.33C-1.50Ni-1.15Cr Fatigue fracture Brittle fracture Intergranular fracture...