Series: ASM Failure Analysis Case Histories
Volume: 1
Publisher: ASM International
Published: 01 December 1992
DOI: 10.31399/asm.fach.v01.c9001129
EISBN: 978-1-62708-214-3
..., would have prevented the failure. Heat-affected zone Low-cycle fatigue Welded joints Welding parameters Weldments Fe-0.25C-1.24Mn-0.62Cr-0.24Mo Fatigue fracture Joining-related failures Background Visual Examination of General Physical Features Testing Procedure and Results...