Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.usage.c9001630
EISBN: 978-1-62708-236-5
... at the same location in almost all the other caps on the same device. The cracking had been in progress for considerable time. Amusement ride Bearing cap Catastrophic failure Octopus Fe-0.41C-0.8Mn Fe-0.25C-0.7Mn Fatigue fracture ...