Skip Nav Destination
Close Modal
Search Results for
Economizers
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-20 of 139 Search Results for
Economizers
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001825
EISBN: 978-1-62708-241-9
...): ×100 Fig. 15 Microstructure and crack morphology in the base metal of the tube away from the header. Etchant: 10% oxalic acid (electrolytic). Magnification: ×100 Abstract A type 304 stainless steel tube that failed in a boiler stack economizer was analyzed to determine the cause...
Abstract
A type 304 stainless steel tube that failed in a boiler stack economizer was analyzed to determine the cause. The investigation consisted of visual, SEM/EDS, and metallographic analysis. Several degradation mechanisms appeared to be at work, including pitting corrosion, chloride stress corrosion cracking, and fatigue fracture. Investigators concluded that the primary failure mechanism was fatigue fracture, although either of the other mechanisms may have eventually caused the tube to fail in the absence of fatigue.
Image
in Alloy 430 Ferritic Stainless Steel Welds Fail due to Stress-Corrosion Cracking in Heat-Recovery Steam Generator
> ASM Failure Analysis Case Histories: Power Generating Equipment
Published: 01 June 2019
Fig. 2 Feedwater economizer, finned tube harp assembly
More
Image
in Cause and Prevention of Fatigue Failures in Boiler Tubing
> ASM Failure Analysis Case Histories: Power Generating Equipment
Published: 01 June 2019
Fig. 14 Configuration & Economizer Note failures were at the bottom portion of the fins and cracking occurred under fin.
More
Image
in Cause and Prevention of Fatigue Failures in Boiler Tubing
> ASM Failure Analysis Case Histories: Power Generating Equipment
Published: 01 June 2019
Fig. 15 Water Side of Economizer Tube - Note cracks under fin area. 3.5×.
More
Image
in Cause and Prevention of Fatigue Failures in Boiler Tubing
> ASM Failure Analysis Case Histories: Power Generating Equipment
Published: 01 June 2019
Fig. 16 Metallographic Specimen Through Cracks in Economizer Tube - Note straight, transgranular, unbranched, oxidized cracks under fin.
More
Image
in Corrosion-Fatigue Failure of Finned Stainless Steel Economizer Tubes Due to Differential Thermal Expansion
> ASM Failure Analysis Case Histories: Pulp and Paper Processing Equipment
Published: 01 June 2019
Fig. 1 Section of stainless steel tube/fin assembly removed from economizer. Note the weld geometry and fin weld locations.
More
Image
in Corrosion-Fatigue Failure of Finned Stainless Steel Economizer Tubes Due to Differential Thermal Expansion
> ASM Failure Analysis Case Histories: Pulp and Paper Processing Equipment
Published: 01 June 2019
Fig. 2 Interior surface of economizer tube after penetrant testing. Note indications of cracking (arrows).
More
Image
in Corrosion-Fatigue Failure of Finned Stainless Steel Economizer Tubes Due to Differential Thermal Expansion
> ASM Failure Analysis Case Histories: Pulp and Paper Processing Equipment
Published: 01 June 2019
Fig. 3 Inside-diameter cracking in stainless steel economizer tube. (a) Cross section of tube near the end of fin fillet weld. Note cracking at the root and toe of the weld. (b) Cross section of tube under unwelded fin end showing crack below fin and pitting on inside-diameter surface. (c
More
Image
in Failure Analysis of Heat Exchangers
> Analysis and Prevention of Component and Equipment Failures
Published: 30 August 2021
Fig. 19 Economizer inlet tube showing open rupture and a hole. Source: Ref 4
More
Image
in Failure Analysis of Heat Exchangers
> Analysis and Prevention of Component and Equipment Failures
Published: 30 August 2021
Fig. 20 Thinning of economizer inlet tube toward the rupture side. Source: Ref 4
More
Image
in Failure of Boilers and Related Equipment
> Analysis and Prevention of Component and Equipment Failures
Published: 30 August 2021
Fig. 39 Erosion-corrosion damage of economizer tube bend
More
Image
in Failure of Boilers and Related Equipment
> Analysis and Prevention of Component and Equipment Failures
Published: 30 August 2021
Fig. 59 Photograph showing close-up view of economizer drain tube, highlighting extensive damage in the form of nonuniform multicolored scale deposits on the outer surface
More
Book Chapter
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.pulp.c0047615
EISBN: 978-1-62708-230-3
... Abstract After ten years of satisfactory operation, economizer-tube failures occurred in a large black liquor recovery boiler for a paper mill. The economizer contained 1320 finned tubes. Two fins ran longitudinally for most of the tube length and were attached by fillet welding on one side...
Abstract
After ten years of satisfactory operation, economizer-tube failures occurred in a large black liquor recovery boiler for a paper mill. The economizer contained 1320 finned tubes. Two fins ran longitudinally for most of the tube length and were attached by fillet welding on one side. The economizer tube leaks occurred at the end of the fin near the bottom of the economizer. A sample from a tube that had not failed showed heavy pitting attack on the inside of the tube, probably due to excess oxygen in the feedwater. Penetrant testing revealed numerous longitudinal cracks on the inside in the area of the fin tip. Cracking at the end of the fin-to-tube fillet weld was noted. The results indicate the failures were due to corrosion fatigue whose stresses were primarily thermally induced. A temporary solution included inspecting all tubes with shear-wave ultrasonics. Tubes with the most severe cracking were ground and repair welded. The square corners of the fins were trimmed back with a gradual taper so that expansion strains would be more gradually transferred to the tube surface. Water chemistry was closely evaluated and monitored, especially with regard to oxygen content.
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.power.c9001569
EISBN: 978-1-62708-229-7
... Abstract This paper reviews several fatigue failures from the waterwall, superheater, and economizer portions of the boiler, their causes and how they were mitigated and monitored. Some cases required simple field modifications by cutting or welding, repair of existing controls, and/or changes...
Abstract
This paper reviews several fatigue failures from the waterwall, superheater, and economizer portions of the boiler, their causes and how they were mitigated and monitored. Some cases required simple field modifications by cutting or welding, repair of existing controls, and/or changes in maintenance. Nondestructive inspections by visual, magnetic particle, ultrasonic, and radiographic methods for detecting and monitoring damage are discussed. These failures are presented to provide hindsight that will help others in increasing the success rate for anticipating and analyzing the remaining life of other units.
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.power.c9001482
EISBN: 978-1-62708-229-7
... Abstract Penetration by molten copper occurred in the economizer of a large water-tube boiler. A cross section through a weld and the crack in the tube revealed a crack was an intergranular fissure. Small fissures of the same type also extended from its flanks. The main fissure was filled...
Abstract
Penetration by molten copper occurred in the economizer of a large water-tube boiler. A cross section through a weld and the crack in the tube revealed a crack was an intergranular fissure. Small fissures of the same type also extended from its flanks. The main fissure was filled with an oxide scale in which were embedded particles having the appearance of metallic copper. It was concluded that the cracking that occurred at the time of re-welding was due to intergranular penetration by copper present in the deposit within the tubes, which had not been completely removed prior to welding. Subsequently, it was ascertained that trouble had been experienced with the centrifugal feed pumps, resulting in scuffing of some bronze rings. The presumption is that bronze particles had been carried in mechanical suspension in the feed water and deposited in the economizer tubes.
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.power.c9001609
EISBN: 978-1-62708-229-7
... of its resistance to chloride and sulfuric acid dewpoint corrosion under conditions potentially present in the HRSG low-pressure feedwater economizer. Intergranular corrosion and cracking were found in the weld metal and heat-affected zones. The hardness in these regions was up to 35 HRC, and the weld...
Abstract
Alloy 430 stainless steel tube-to-header welds failed in a heat recovery steam generator (HRSG) within one year of commissioning. The HRSG was in a combined cycle, gas-fired, combustion turbine electric power plant. Alloy 430, a 17% Cr ferritic stainless steel, was selected because of its resistance to chloride and sulfuric acid dewpoint corrosion under conditions potentially present in the HRSG low-pressure feedwater economizer. Intergranular corrosion and cracking were found in the weld metal and heat-affected zones. The hardness in these regions was up to 35 HRC, and the weld had received a postweld heat treatment (PWHT). Metallographic examination revealed that the corroded areas contained undertempered martensite. Fully tempered weld areas with a hardness of 93 HRB were not attacked. No evidence of corrosion fatigue was found. Uneven temperature control during PWHT was the most likely cause of failure.
Book Chapter
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.process.c0059924
EISBN: 978-1-62708-235-8
... was the most economical solution. Billets Nonmetallic inclusions Rings Ultrasonic testing 8822 UNS G88220 Metalworking-related failures The large steel ring shown in Fig. 1 was produced for a nuclear application from a 1.7 in (68 in.) diam billet of 8822 steel. The large billet was first...
Abstract
The large steel ring produced for a nuclear application from a billet of 8822 steel was inspected. The large billet was first forged into a doughnut preform in a large press, and then formed into the ring by ring rolling. A straight-beam ultrasonic inspection was instituted and calibrated using the back-surface-reflection method to determine whether adequate ultrasonic penetration was available. Areas of indications were noted at approximately midheight and adjacent to the bore area. An axial angle-beam inspection from the outside was performed, mainly in the area of indications to reveal detectable indications. The indications were not considered serious enough to reject the forgings. A few small indications in the areas tested were revealed by magnetic particle inspection. The area was conditioned by grinding and polishing to obtain an additional inspection at a greater depth from the inside surface. A much more severe condition was revealed after the test. The indications were classified as areas of chemical segregation and nonmetallic inclusions. The ring was considered unsatisfactory for the application and replacement of the defective ring from an acceptable billet was the most economical solution.
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.process.c9001601
EISBN: 978-1-62708-235-8
... Abstract Flow forming technology has emerged as a promising, economical metal forming technology due to its ability to provide high strength, high precision, thin walled tubes with excellent surface finish. This paper presents experimental observations of defects developed during flow forming...
Abstract
Flow forming technology has emerged as a promising, economical metal forming technology due to its ability to provide high strength, high precision, thin walled tubes with excellent surface finish. This paper presents experimental observations of defects developed during flow forming of high strength SAE 4130 steel tubes. The major defects observed are fish scaling, premature burst, diametral growth, microcracks, and macrocracks. This paper analyzes the defects and arrives at the causative factors contributing to the various failure modes.
Book Chapter
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.bldgs.c9001457
EISBN: 978-1-62708-219-8
... Abstract The cover of a feed cock fitted to an economic boiler suddenly blew off and the plug lifted sufficiently to permit the escape of water. It was found that all four of the studs securing the cover had fractured. In each case fracture had occurred at the end of one of the screwed portions...
Abstract
The cover of a feed cock fitted to an economic boiler suddenly blew off and the plug lifted sufficiently to permit the escape of water. It was found that all four of the studs securing the cover had fractured. In each case fracture had occurred at the end of one of the screwed portions adjacent to the shank. The fractures were of a short nature, with no evidence of progressive cracking by fatigue, nor was there any sign of stretching prior to failure. The fractured faces and the shanks of the studs were of rusted appearance. Microscopic examination of the material showed it to be an austenitic nickel-chromium stainless steel, stabilized by titanium and of the free machining type. Multiple transgranular cracking characteristic of failure from stress-corrosion cracking, was present to an extensive degree. It was considered probable that there had been slight leakage of water from the valve over a period and evaporation resulted in a solution which favored failure from stress-corrosion cracking. If corrosion resistant studs were desired, those of bronze or Monel metal are to be preferred.
Image
in Failure of Boilers and Related Equipment
> Analysis and Prevention of Component and Equipment Failures
Published: 30 August 2021
Fig. 58 Suggested minimum metal temperatures to avoid flue-gas corrosion in economizers and air heaters plotted as a function of as-fired sulfur contents of various fuels
More
1