EISBN: 978-1-62708-214-3
... Abstract A catastrophic brittle fracture occurred in a welded steel (ASTM A517 grade H) trapezoidal cross-section box girder while the concrete deck of a large bridge was being poured. The failure occurred across the full width of a 57 mm (2 1 4 in.) thick, 760 mm (30 in.) wide flange...
Series: ASM Failure Analysis Case Histories
Volume: 2
Publisher: ASM International
Published: 01 December 1993
DOI: 10.31399/asm.fach.v02.c9001268
EISBN: 978-1-62708-215-0
... Abstract A missile detached from a Navy fighter jet during a routine landing on an aircraft carrier deck because of a faulty missile launcher detent spring. Visual inspection of Inconel 718 detent spring assembly revealed that four of the nine spring leafs comprising the assembly were...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001814
EISBN: 978-1-62708-241-9
... gasifier was examined. The vessel shell was bulged and had ruptured on the east side at the seventh deck level. Figure 3 shows the rupture from the south, which was 17 in. below the transition from the combustion chamber to the quench chamber. The rupture allowed hot gas to escape, and a fire occurred on...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001759
EISBN: 978-1-62708-241-9
... diameter. Heat treatment: liquid nitriding Furnace used: Deck India Engineering Pvt Ltd. Push-out load was measured by resting the bearing cup on locator. Load was applied gradually through rotary actuator. The bearing cup tested by push-out load test. Bearing cup was found to...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.design.c9001578
EISBN: 978-1-62708-233-4
... synchronous, which means that all the units operated at exactly the same speed—in this case, 1200 rpm. To make the situation worse, all the motor generator sets were located on the same metal deck. There was a total of 30 rotating elements (five synchronous motors and 25 generators) operating on one metal...
Book Chapter

Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006790
EISBN: 978-1-62708-295-2
..., and in pipes and screen decks in some screening applications ( Ref 10 ). Table 1 summarizes each of these classifications in terms of the abrasive size, the nature of contact, and the environmental factors. Figure 3 shows in schematic form the four classifications. All of these mechanisms are...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006778
EISBN: 978-1-62708-295-2
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006783
EISBN: 978-1-62708-295-2