Series: ASM Failure Analysis Case Histories
Volume: 2
Publisher: ASM International
Published: 01 December 1993
DOI: 10.31399/asm.fach.v02.c9001355
EISBN: 978-1-62708-215-0
... that the sources of the chlorides be eliminated and that the remaining blades be inspected at regular maintenance intervals for evidence of cracking. Chlorides Environmental effects Mechanical properties Turbine blades DIN X20Cr13 Fatigue fracture Corrosion fatigue Pitting corrosion Background...