Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.modes.c0060144
EISBN: 978-1-62708-234-1
... caused by third-stage creep in tubes because of the cost involved in removing the catalysts. Cracking (fractoring) Radiography Reformer furnaces Tubes HK-40 UNS J94204 Creep fracture/stress rupture ( Ref 1 ). About 1 year after start-up, two steam-methane reformer furnaces were subjected...