Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.modes.c9001674
EISBN: 978-1-62708-234-1
...Abstract Abstract Accelerated aging tests on detonator assemblies, to verify the compatibility of gold bridgewire and Pd-In-Sn solder with the intended explosives, revealed an unusual form of corrosion. The tests, conducted at 74 deg C (165 deg F) and 54 deg C (130 deg F), indicated...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.process.c0049796
EISBN: 978-1-62708-235-8
...Abstract Abstract Problems with materials compatibility were encountered in pyrotechnically driven devices used in a number of ordnance applications requiring rapid mechanical actuation. A fine bridgewire is located in contact with the chemical pyrotechnic, and the charge is ignited...