1-17 of 17 Search Results for

Black liquor

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.pulp.c9001564
EISBN: 978-1-62708-230-3
... Abstract An 8 in. diam stainless steel black liquor feed pipe to a carbon steel digester had failed within one year of service. The material was type 316 molybdenum-containing austenitic stainless steel. The service environment was alkaline black liquor at 175 deg C (350 deg F). The pipe had...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.pulp.c9001567
EISBN: 978-1-62708-230-3
... Abstract A falling film black liquor evaporator consisted of flat twin plate heat exchangers and was used to increase black liquor solids content prior to its burning in the recovery boiler. Several plate heat exchangers were fabricated of AISI type 316L stainless steel by electric resistance...
Series: ASM Failure Analysis Case Histories
Volume: 2
Publisher: ASM International
Published: 01 December 1993
DOI: 10.31399/asm.fach.v02.c9001311
EISBN: 978-1-62708-215-0
... Abstract Several nickel-base superalloy (UNS N06600) welded heat-exchanger tubes used in processing black liquor in a kraft paper mill failed prematurely. Leaking occurred through the tube walls at levels near the bottom tube sheet. The tubes had been installed as replacements for type 304...
Series: ASM Failure Analysis Case Histories
Volume: 1
Publisher: ASM International
Published: 01 December 1992
DOI: 10.31399/asm.fach.v01.c9001049
EISBN: 978-1-62708-214-3
..., which are natural components of wood. The batch process begins with filling the vessel ( Fig. 1 ) with wood chips and white and black liquor. This slurry is heated to 205 °C (400 °F) under a pressure of 965 kPa (140 psi) for approximately 2 1 2 h. The digested material is then discharged...
Image
Published: 01 June 2019
Fig. 1 Cracks at the inside surface of the black liquor pipe were coincident with an external support gusset. More
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.pulp.c0047615
EISBN: 978-1-62708-230-3
... Abstract After ten years of satisfactory operation, economizer-tube failures occurred in a large black liquor recovery boiler for a paper mill. The economizer contained 1320 finned tubes. Two fins ran longitudinally for most of the tube length and were attached by fillet welding on one side...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006812
EISBN: 978-1-62708-329-4
... is shown in Fig. 11 . Figure 12 again shows the cutout near the nozzle ( Fig. 12a ) and the extracted metal part ( Fig. 12b ). The circular black marking on the extracted metal surface ( Fig. 12b ) is due to an attempt to extract a smaller section using a mechanical tool. This attempt had failed because...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006825
EISBN: 978-1-62708-329-4
... processes of gas turbines, diesel engines, or other industrial processes is effectively used to produce hot water or steam to improve the process economy. The kraft-recovery boilers (also known as black-liquor-recovery boilers) produce steam that can be used in the kraft process to generate electricity...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0001816
EISBN: 978-1-62708-180-1
... Microstructures of specimens from carbon steel boiler tubes subjected to prolonged overheating below Ac 1 . (a) Voids (black) in grain boundaries and spheroidization (light, globular), both of which are characteristic of tertiary creep. 250×. (b) Intergranular separation adjacent to fracture surface (top). 50...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003508
EISBN: 978-1-62708-180-1
... are used Blacking scab, wash scab D 240: Oxides adhering after heat treatment (annealing, tempering, malleablizing) by decarburization D 241 Adherence of oxide after annealing Oxide scale D 242 Adherence of ore after malleablizing (white heart malleable Adherent packing material...
Book Chapter

Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003548
EISBN: 978-1-62708-180-1
... by metal dissolution or oxidation. The more cathodic material is more corrosion resistant (i.e., more noble). Fig. 3 Galvanic series of metals and alloys in seawater. Alloys are listed in order of the potential they exhibit in flowing seawater; those indicated by the black rectangle were tested...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006831
EISBN: 978-1-62708-329-4
... scab D 233 (a) Flat, metallic projections on the casting where mold or core washes or dressings are used Blacking scab, wash scab D 240 Oxides adhering after heat treatment (annealing, tempering, malleablizing) by decarburization D 241 Adherence of oxide after annealing Oxide...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006783
EISBN: 978-1-62708-295-2
... by a black rectangle were tested in low-velocity or poorly aerated water and at shielded areas may become active and exhibit a potential near −0.5 V. SCE, saturated calomel electrode. Adapted from Ref 2 Although the measurement of potentials has limitations as previously noted, galvanic series based...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006785
EISBN: 978-1-62708-295-2
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.9781627083294
EISBN: 978-1-62708-329-4
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003553
EISBN: 978-1-62708-180-1
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006808
EISBN: 978-1-62708-329-4