Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.modes.c9001734
EISBN: 978-1-62708-234-1
... become almost routine. Occasionally, opportunities arise in which a unique fracture occurs and lends itself to study on the SEM. This paper concerns the surface appearance and micro features found on the failed cross section of a 2024-T62 aluminum actuator arm which had broken during an intense localized...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.aero.c9001504
EISBN: 978-1-62708-217-4
... opposite to the first one, indicating reversed bending conditions on the trunnion where an assembly arm, linking the end of the steering actuator and the upper torque arm, fitted. The fracture mechanics analysis of the failure showed that the fatigue crack size was critical for normal operating condition...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003566
EISBN: 978-1-62708-180-1
... emitter and detector scans the rim of the disk, and when the slot passes between them, the solenoid is actuated, but only when the manual firing button is pressed. In the photograph, the slot can be seen at the bottom edge of the disk just leaving the detector as the arm carrying the specimen has just...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003508
EISBN: 978-1-62708-180-1
... was submitted for failure analysis to determine the cause of cracking. Investigation The cylinder head was magnetic-particle inspected by both the head and coil methods. No indications were present on the cylinder head, except those shown in Fig. 1 and 2 . The head was cracked on the rocker-arm pan...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006815
EISBN: 978-1-62708-329-4
... sizing and strength. All design features, such as variable vane actuation systems, rotor tip seal active clearance control, piping, and services, are proposed. Purchased items, such as bearings, seals, and lube oil pumps, are coordinated with vendors to provide engineering justification for the size...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006831
EISBN: 978-1-62708-329-4
...-particle inspected by both the head and coil methods. No indications were present on the cylinder head, except those shown in Fig. 2 and 3 . The head was cracked on the rocker-arm pan rail next to the No. 3 intake port. The crack extends into the water jacket on the rocker-arm side of the head. Visual...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.9781627083294
EISBN: 978-1-62708-329-4
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006864
EISBN: 978-1-62708-395-9
... with an encoding device. Common cutting units include swing arm blades, flywheel cutters, or rotary saws. Fig. 15 Face plates, vacuum plates, and shaping plates of a hollow profile process Fig. 16 Setup of a profile extrusion line. Adapted from Ref 1 Mixing and Compounding In most...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.9781627083959