1-20 of 277 Search Results for

ASTM designations

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.process.c0048733
EISBN: 978-1-62708-235-8
... side, 1035 kPa (150 psi) and 185 °C (365 °F). Both sides were hydrostatically tested at 150% of design pressure. The heater tubes were made of copper alloy C70600 (copper nickel, 10%) per ASTM B 466. On-site and laboratory investigations were conducted to determine the cause of failure...
Series: ASM Failure Analysis Case Histories
Volume: 1
Publisher: ASM International
Published: 01 December 1992
DOI: 10.31399/asm.fach.v01.c9001065
EISBN: 978-1-62708-214-3
...Abstract Abstract A 460 mm (18 in.) diam suction line to the main feed water pump for a nuclear power plant failed in a violent, catastrophic manner. Samples of pipe, elbow, and weld materials (ASTM A106 grade B carbon steel, ASTM A234 grade WPB carbon steel, and E7018 carbon steel electrode...
Series: ASM Failure Analysis Case Histories
Volume: 2
Publisher: ASM International
Published: 01 December 1993
DOI: 10.31399/asm.fach.v02.c9001272
EISBN: 978-1-62708-215-0
... of the steel at the time of collapse was estimated to be −1 to 4 °C (30 to 40 °F). Material: ASTM A446 grade B or F steel sheet, zinc-coated by the hot-dip process, structural quality Design Code: German: Silo code DIN 1055 E and DIN 1055 F. U.S.: Janssen theory The design and erection of smaller...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.power.c0048747
EISBN: 978-1-62708-229-7
.... ASTM A53 (Nonresulfurized carbon steel) UNS K03005 Fatigue fracture Joining-related failures Joint design was responsible for mechanical notches at welds in a heat-exchanger component ( Fig. 1 ). A 455 mm (18 in.) diameter, 8 mm ( 5 16 in.) wall carbon steel discharge line...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.process.c0090974
EISBN: 978-1-62708-235-8
... inclusion morphology, and reevaluation of the casting design was suggested to minimize shrinkage. Brackets Castings Inclusions Manganese sulfide Shrinkage ASTM A148 grade 135-125 UNS D51250 Casting-related failures Brittle fracture A cast steel bracket manufactured in accordance with ASTM...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.auto.c0089572
EISBN: 978-1-62708-218-1
...Abstract Abstract Two sand-cast low-alloy steel equalizer beams (ASTM A 148, grade 105-85) designed to distribute the load to the axles of a highway truck broke after an unreported length of service. Normal service life would have been about 805,000 km (500,000 mi) of truck operation...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.process.c0046210
EISBN: 978-1-62708-235-8
... designation AFNOR 38CD4 (similar to AISI type 4140H) and was in the quenched-and-tempered condition, with a yield strength of about 760 MPa (110 ksi). It was treated to have compressive surface stresses, and the prior-austenite grain size was ASTM 8. Analysis (visual inspection, stress analyses...
Series: ASM Failure Analysis Case Histories
Volume: 1
Publisher: ASM International
Published: 01 December 1992
DOI: 10.31399/asm.fach.v01.c9001055
EISBN: 978-1-62708-214-3
... lines. Certified test results from the steel mill, procedure qualification tests of the welding, and design changes to reduce water hammer were also recommended. Impact toughness Notch sensitivity Pipe joints Pipe Water pipelines Welding parameters ASTM A283 grade D UNS K02702 Joining...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.bldgs.c9001135
EISBN: 978-1-62708-219-8
... rates in the banded region. By noting these differences, bridge engineers can re-evaluate existing designs and modify current bridge inspection procedures. The steel used in the construction of this bridge was specified as ASTM A441, a steel commonly used in structural applications. Normally...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.modes.c0047879
EISBN: 978-1-62708-234-1
... was made of ASTM A105, grade 2 steel, and the larger-diameter section was covered with a type 316 stainless steel end cap. The cap was secured at each end by welding, using type ER316 stainless steel filler metal (Detail A, “Original design,” Fig. 1 ). The radial surface at the change in diameter...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006761
EISBN: 978-1-62708-295-2
... Mechanical Testing Definitions and Basics Strength/Ductility Testing Acknowledgments References References 1. “ Standard Test Methods for Tension Testing of Metallic Materials ,” E 8/E8M-16, ASTM International 2. “ Standard Test Method for Guided Bend Test for Ductility of Welds ,” E 190...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.9781627082952
EISBN: 978-1-62708-295-2
Series: ASM Failure Analysis Case Histories
Volume: 1
Publisher: ASM International
Published: 01 December 1992
DOI: 10.31399/asm.fach.v01.c9001120
EISBN: 978-1-62708-214-3
... chemical analysis was conducted on the segment. The composition is shown in Table 1 . Based on the chemical analysis, the die complied with the chemical requirements for ASTM A681-89 H13 tool steel (see Table 1 ). Composition of the fractured segment, compared with that of the designated tool steel...
Series: ASM Failure Analysis Case Histories
Volume: 1
Publisher: ASM International
Published: 01 December 1992
DOI: 10.31399/asm.fach.v01.c9001108
EISBN: 978-1-62708-214-3
.... fabricator corresponded to ASTM B 407. Technical information from internationally known petrochemical industries based on their long-term experience with reformer furnaces indicates that problems in high-nickel alloy pigtails can he associated with cold-work procedures ( Ref 1 ). For instance...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001777
EISBN: 978-1-62708-241-9
... ksi Minimum Tensile Strength . ASTM International , West Conshohocken ( 2011 ) 12. AISC S342. Load and Resistance Factor Design Specification for Structural Steel Buildings . American Institute of Steel Construction , Chicago ( 1993 ) 13. ASTM A36/A36M-08. Standard Specification...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.steel.c9001668
EISBN: 978-1-62708-232-7
... as a result of the analysis. Autoclaves Bolts Design Explosions ASTM A449 (Other, miscellaneous, or unspecified) failure Failure analysis is much more than just a metallurgical and fractographic examination combined with the measurement of a few mechanical properties. Failure analysis...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0001819
EISBN: 978-1-62708-180-1
..., such as fatigue. Design of Internal Fixation Devices Leading internal fixation systems contain different types of devices that are available in various configurations and sizes. Some major implant types are specified by standard-bearing organizations, such as ASTM and ISO, but many established implants...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.matlhand.c0048064
EISBN: 978-1-62708-224-2
...) Macrograph of a nital-etched section showing cracks propagating from the surface (top), which was hardened and embrittled during torch cutting. 7 1 2 ×. (c) Replacement hook of a laminated design made of ASTM A242 fine-grain steel plate. Dimensions given in inches Macroscopic examination...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.bldgs.c9001697
EISBN: 978-1-62708-219-8
... water Water treatment C12200 UNS C12200 ASTM B88 UNS C12200 Pitting corrosion Potable waters are defined as waters that are suitable for drinking purposes. Potable waters are in use throughout the United States and new systems are being installed on a daily basis. The quality of potable...
Series: ASM Failure Analysis Case Histories
Volume: 2
Publisher: ASM International
Published: 01 December 1993
DOI: 10.31399/asm.fach.v02.c9001284
EISBN: 978-1-62708-215-0
... AM60A (ASTM B94). Surface Examination Metallography Chemical Analysis/Identification Examination revealed that the stock riser had cold shuts present at the site where fracturing occurred on the other risers. Cold shuts occur during the casting process as metal flows into the mold and fails...