1-3 of 3 Search Results for

ASTM B337 grade 2

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.modes.c0048757
EISBN: 978-1-62708-234-1
...Abstract Abstract Brief overheating of the 89 mm OD 6.4 mm wall thickness titanium heater tubes (ASTM B337, grade 2) was caused by a flow stoppage in a leach heater. Blue-tinted areas and patches of flaky white, yellow, and brown oxide scale was revealed on visual examination. It was disclosed...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0001817
EISBN: 978-1-62708-180-1
... at welded joints because of overstress during normal operation. Dimensions given in inches Fig. 15 Titanium heat-exchanger tube (ASTM B337, grade 2) that became embrittled and failed because of absorption of hydrogen and oxygen at elevated temperatures. (a) Section of the titanium tube...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006813
EISBN: 978-1-62708-329-4
... the surface that was denickelified (top) and unaffected base metal (bottom). Etched with equal parts nitric and acetic acid. Original magnification: 375├Ś Fig. 16 Titanium heat-exchanger tube (ASTM B337, grade 2) that became embrittled and failed because of absorption of hydrogen and oxygen...