Series: ASM Failure Analysis Case Histories
Volume: 2
Publisher: ASM International
Published: 01 December 1993
DOI: 10.31399/asm.fach.v02.c9001325
EISBN: 978-1-62708-215-0
... quality. Hydrogen sulfide Weld metal Welded joints UNS K03005 UNS K03504 UNS K03006 ASTM A53 grade B ASTM A105 ASTM A234 grade WPB Uniform corrosion High-temperature corrosion and oxidation Background Visual Examination of General Physical Features Testing Procedure and Results...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006812
EISBN: 978-1-62708-329-4
... was 900 °C (1650 °F). Fig. 5 Return bend made of ASTM A213, grade T11, ferritic steel that ruptured because it contained a large number of inclusions. (a) Overall view of the return bend showing rupture. (b) Micrograph of an unetched specimen showing high concentration of inclusions. Original...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0001818
EISBN: 978-1-62708-180-1
... a hydrostatic test because it had cracked in the weld. Analysis showed that the cap had a carbon content of 0.56%, whereas a maximum carbon content of 0.30% was specified. The excessive carbon content had resulted in a brittle HAZ. It was found that construction personnel had substituted ASTM A53 type F butt...