Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.conag.c0047474
EISBN: 978-1-62708-221-1
... Abstract A 10-cm (4-in.) chain link used in operating a large dragline bucket failed after several weeks in service. The link was made of cast low-alloy steel (similar to ASTM A487, class 10Q) that had been normalized, hardened, and tempered to give a yield strength of approximately 1034 MPa...