EISBN: 978-1-62708-215-0
... mechanics Fracture toughness Galvanized steels Mechanical properties Stresses Tanks ASTM A446 grade B ASTM A446 grade F Brittle fracture Background A large grain bin failed cataclysmically soon after erection ( Fig. 1 , 2 ). Failure occurred while the bin was in the static loaded condition...