... Abstract A vessel made of ASTM A204, grade C, molybdenum alloy steel and used as a hydrogen reformer was found to have cracked in the weld between the shell and the lower head. Six samples from different sections were investigated. The crack was found to be initiated at the edge of the weld in...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.chem.c0048835
EISBN: 978-1-62708-220-4
... were found in longitudinal and circumferential seam welds of the 113-mm (4 7 16 -in.) thick ASTM A204, grade A, Fe-C-0.5Mo steel sheel. Indications were also found in the 57-mm (2 1 4 -in.) thick top and bottom heads that were formed by welding pie sections of plate. No records were...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0001818
EISBN: 978-1-62708-180-1
...) entering at 260 to 290 °C (500 to 550 °F) and leaving at 425 to 480 °C (800 to 900 °F). The temperature of the combustion gas was 900 °C (1650 °F). Fig. 3 Return bend made of ASTM A213, grade T11, ferritic steel that ruptured because it contained a large number of inclusions. (a) Overall view of the...