Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001776
EISBN: 978-1-62708-241-9
... that the precipitation of carbides at the grain boundaries may have occurred because of improper heat treatment, but not because of a deficiency in composition. crusher jaws fracture embrittlement steel grainy surface texture metallographic analysis impact strength ASTM A 128 grade B-4 (austenitic manganese...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.chem.c9001534
EISBN: 978-1-62708-220-4
... 10, ASTM , 1980 , p 197 – 212 4. Standard Methods for Mechanical Testing of Welds, ANSI/AWS B 4.0-85 , American Welding Society , Florida , 1985 , p 31 – 37 5. Lancaster J.F. , Metallurgy of Welding , 3rd ed. , George Allen & Unwin , London , 1980 , p 128 – 129...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006812
EISBN: 978-1-62708-329-4
... was 900 °C (1650 °F). Fig. 5 Return bend made of ASTM A213, grade T11, ferritic steel that ruptured because it contained a large number of inclusions. (a) Overall view of the return bend showing rupture. (b) Micrograph of an unetched specimen showing high concentration of inclusions. Original...
Book Chapter

Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003548
EISBN: 978-1-62708-180-1
... through a conducting medium or electrolyte to the other more cathodic metal (liberating hydrogen and/or causing a “reduction” of oxides). This action is seen in Fig. 2 where a couple is made up of steel and mill scale. Fig. 2 Breaks in mill scale (Fe 3 O 4 ) leading to galvanic corrosion of steel...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006783
EISBN: 978-1-62708-295-2
...). This action is seen in Fig. 2 where a couple is made up of steel and mill scale. Fig. 2 Breaks in mill scale (Fe 3 O 4 ) leading to galvanic corrosion of steel The three essential components for galvanic corrosion are: Materials possessing different surface potential A common...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006808
EISBN: 978-1-62708-329-4
... Schematic of defects and discontinuities in welded joints Fig. 4 Weld discontinuities affecting weld shape and contour. (a) Undercut and overlap in a fillet weld. (b) Undercut and overlap in a groove weld. (c) and (d) Underfill in groove welds Fig. 5 Identification of cracks according...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006788
EISBN: 978-1-62708-295-2
.... , and Spear J.R. , Microbially Influenced Corrosion Communities Associated with Fuel-Grade Ethanol Environments , Appl. Microbiol. Biotechnol. , Vol 99 ( No. 16 ), 2015 , p 6945 – 6957 10.1007/s00253-015-6729-4 54. Little B. , Staehle R. , and Davis R. , Fungal Influenced...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006792
EISBN: 978-1-62708-295-2
.... , Miedema K. , Scheetz J. , and Williams J. , Introduction of Nitrided M50 and M50NiL Bearings into Jet Engine Mainshaft Applications , Bearing Steel Technologies: Tenth Volume, Advances in Steel Technologies for Rolling Bearings , Beswick J. , Ed., ASTM International , West...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006787
EISBN: 978-1-62708-295-2
... designation Maximum temperature Ref °C °F Carbon and alloy steels AISI 1010 carbon steel 480 895 3 SA-178, grade A 510 (a) 950 (a) 4 SA-192; SA-210, grade A 510 (a) 950 (b) 4 SA-209, grade T-1A 525 (b) 975 (b) 4 1Cr-Mo-Si; SA-213, grade T-11 565...