... monitoring and maintenance to ensure that another low-pH excursion does not occur. Boiler tubes Chlorides, environment ASME SA210-C Pitting corrosion Background Testing Procedure and Results Discussion Conclusion and Recommendations Selected Reference Selected Reference • Forms...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.power.c9001709
EISBN: 978-1-62708-229-7
... at 693 deg F (367 deg C) and 2935 psi (20.5 MPa), failed near the IK boxes as a result of thermal fatigue. Thermal fatigue damage was accelerated by repetitive exposure to water droplets from the soot blower and the associated rapid cooling. Boilers Electric power generation Tubes ASME SA210-A1...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006825
EISBN: 978-1-62708-329-4
... applications Table 2 Chemical composition of alloys used in subcritical boiler-related applications Grade specifications C Si Mn Cr Ni Mo V Nb Others Remarks SA210 grade A1 0.27 max 0.10 min 0.93 max … … … … … 0.035 max S and P … SA210 grade C 0.35...