Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001821
EISBN: 978-1-62708-241-9
... large grain structure continuous transverse grain boundaries microstructural analysis ultimate tensile strength A202B (chromium-manganese-silicon alloy steel) Background Failure Investigation of Excess Flow Valves on Stationary Tank BLEVE of Truck-Mounted Tank Discussion of BLEVE...