Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.steel.c9001598
EISBN: 978-1-62708-232-7
.... In addition, the use of grain stabilized Pt/Rh alloy should be evaluated as a method to prevent grain growth. Wall thinning 80Pt-20Rh Pitting corrosion Creep fracture/stress rupture Background Americium and Curium (Am-Cm) were recovered in one of the Savannah River Site's (SRS) two chemical...