... ] The investigated failed bars are made of spring steel. The spring steel (50CrV4, EN10132-4) is a heat-treatable alloy material. Two bars are damaged virtually every month in textile factory and the damage and resulting machine downtime resulted in significant loss of production. Therefore, the damaged torsion bars...