Fig. 1 Typical microstructure of a 50Ag50Mo contact. The light areas are silver, the dark areas molybdenum. 380× More
Series: ASM Failure Analysis Case Histories
Volume: 2
Publisher: ASM International
Published: 01 December 1993
DOI: 10.31399/asm.fach.v02.c9001389
EISBN: 978-1-62708-215-0
..., and calibration areas be isolated from molding areas. Ammonia, environment Atmospheric corrosion Circuit breakers Electric contacts, corrosion Electrical resistance 50Ag-50Mo 73W-27Ag Uniform corrosion Background During routine quality control testing, electrical switchgear devices exhibited...