Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001799
EISBN: 978-1-62708-241-9
... the bearings led to the transfer of material. gear shaft fatigue fracture seizing high-strength low-alloy steel scoring marks deformed grains uniaxial fatigue testing macrofeatures 4145 (high-strength low-alloy steel) UNS G41450 Introduction Service History Observations and Analyses...