Published: 01 June 2019
Fig. 1 Cast of 357 aluminum, these racing car engine pistons became severely damaged during a 500 mile race. Number 1 has a crumbly deposit on the crown; No. 2 and 3 have carbonaceous deposits; and No. 4 is badly dented. More
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.auto.c9001543
EISBN: 978-1-62708-218-1
... Abstract To determine the effect of severe service on cast 357 aluminum pistons, a metallurgical evaluation was made of four pistons removed from the engine of the Hawk-Offenhauser car which had been driven by Rich Muther in the first Ontario, California 500 race. The pistons were studied...
Image
Published: 01 December 2019
Fig. 11 Microhardness values in different zones of weld joint as taken on reference specimen, i.e. without cracks, are (a) weld zone 345–355 HV, (b) HAZ 357–367 HV, (c) HAZ on opposite side of weld bead 353–367 HV, (d) base metal 346–357 HV and (e) base metal on opposite side of weld bead 347 More
Image
Published: 01 June 2019
Fig. 3 Temperatures developed in racing were high enough to melt out low-melting-point material in the 357 alloy, leaving porous zones in piston crowns. Such structures appear as shrinkage porosity in radiographs. Unetched; 35×. More
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001837
EISBN: 978-1-62708-241-9
... on reference specimen, i.e. without cracks, are (a) weld zone 345–355 HV, (b) HAZ 357–367 HV, (c) HAZ on opposite side of weld bead 353–367 HV, (d) base metal 346–357 HV and (e) base metal on opposite side of weld bead 347–358 HV Fig. 12 Microhardness values in different zones of weld joint...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001804
EISBN: 978-1-62708-241-9
... of steels . Mater. Charact. 36 , 357 – 364 ( 1996 ) 10.1016/S1044-5803(96)00070-8 14. ASM Handbook, Failure Analysis and Prevention , volume 11 , ( ASM International , Materials Park , 2004 ), p. 1164 15. ASM Handbook, Volume 1, Properties and Selection: Irons, Steels and High...
Series: ASM Failure Analysis Case Histories
Volume: 2
Publisher: ASM International
Published: 01 December 1993
DOI: 10.31399/asm.fach.v02.c9001388
EISBN: 978-1-62708-215-0
... of a failed bolt. Hardness ranged from 357 to 381 HV. Tensile Properties Based on the Vickers hardness results, the tensile strength of the bolt material was approximately 1200 MPa (175 ksi). Fatigue Properties Fatigue testing of an unfailed bolt was performed under tension-tension cyclic...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001791
EISBN: 978-1-62708-241-9
... 11. Baxter D.F. Jr. (ed.): ASM Handbook—Fractography , vol. 12 . ASM International , Materials Park ( 1987 ) 12. Wouters R. , Froyen L. : Scanning electron microscope fractography in failure analysis of steels . Mater. Charact. 36 , 357 – 364 ( 1996 ) 10.1016...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001819
EISBN: 978-1-62708-241-9
... ) (in Portuguese) 14. Wouters R. , Froyen L. : Scanning electron microscope fractography in failure analysis of steels , Mater. Charact. , 36 , 357 – 364 ( 1996 ) 10.1016/S1044-5803(96)00070-8 15. Properties and Selection : Stainless Steels , Tool Materials and Special-Purpose...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003564
EISBN: 978-1-62708-180-1
.... , The Hertzian Cone Crack , J. Appl. Mech. (Trans. ASME) , Vol 58 , 1991 , p 120 – 127 17. Warren P.D. , Hills D.A. , and Dai D.N. , Mechanics of Hertzian Cracking , Tribol. Int. , Vol 28 , 1995 , p 357 – 362 18. Suh N.P. , An Overview of the Delamination Theory...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.med.c9001606
EISBN: 978-1-62708-226-6
... and Properties of Engineering Materials , McGraw-Hill , New York, NY , 2002 , pp. 255 and 357 . 17. Anon .: ABAQUS User's Manual , Version 6.2, Hibbit, Karlsson, and Sorenson, Inc. , Providence, RI , 2001 , pp. 14.1.1 – 2 . 18. Hughes T.J.R. : The Finite Element Method , Prentice...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001839
EISBN: 978-1-62708-241-9
... J.A. , Rawl D.E. , Mater. Sci. Eng . 10 , 357 – 368 ( 1972 ) 10.1016/0025-5416(72)90109-7 4. Odegard B.C. , Brooks J.A. , West A.J. , The effect of hydrogen on mechanical behavior of nitrogen-strengthened stainless steel , in Proceedings of International Conference...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006914
EISBN: 978-1-62708-395-9
... for selected polymers from ASTM D1929 Table 1 Flash-ignition and self-ignition temperatures for selected polymers from ASTM D1929 Polymer Flash-ignition Self-ignition °C °F °C °F Polyethylene (PE) 341–357 646–674 349 660 Polyvinyl chloride (PVC) 391 736 454 849...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006826
EISBN: 978-1-62708-329-4
... , American Society for Metals , 1986 , p 362 8. Finn M.E. and Pfeiffer J.R. , Surface Integrity , Third International Conference on the Behaviour of Materials in Machining , Institute of Materials, University of Warwick , U.K. , Nov 1994 , p 354 , 357 9. Field M...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003514
EISBN: 978-1-62708-180-1
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006792
EISBN: 978-1-62708-295-2
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003571
EISBN: 978-1-62708-180-1
...,” paper 720449, Society of Automotive Engineers , 1971 26. Lancaster J.K. and Giltrow J.P. , The Role of the Counterface Roughness in the Friction and Wear of Carbon Fibre Reinforced Thermosetting Resins , Wear , Vol 16 , 1970 , p 357 – 374 27. Bhushan B. and Wilcock...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006850
EISBN: 978-1-62708-395-9
... 16 , 1970 , p 357 – 374 10.1016/0043-1648(70)90102-X 26. Bhushan B. and Wilcock D.F. , Wear Behaviour of Polymeric Compositions in Dry Reciprocating Sliding , Wear , Vol 75 , 1982 , p 41 – 70 10.1016/0043-1648(82)90139-9 27. Briscoe B.J. , Ramirez I...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006936
EISBN: 978-1-62708-395-9
.... Brunner, Retired Scientist, Empa, Switzerland. References References 1. Brunner A.J. , Hack E. , and Neuenschwander J. , Nondestructive Testing , in Characterization and Analysis of Polymers , Seidel A. , Ed., J. Wiley & Sons , 2008 , p 357 – 377 2...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006764