Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.chem.c9001403
EISBN: 978-1-62708-220-4
... distributing units Heating coils Vessels 18Cr-8Ni-3Mo Stress-corrosion cracking Transgranular fracture This case study concerns a process vessel heating coil, which was fabricated from 3 in. O.D. ├Ś 12 s.w.g. austenitic stainless steel. The coil consisted of several 3 ft. diameter turns...