Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.chem.c9001161
EISBN: 978-1-62708-220-4
... 12CrMo19 5 Joining-related failures Hydrogen damage and embrittlement A heat exchanger was removed from an ammonia synthesis plant after five years' service because loss of gas indicated a leak. The container consisted of a number of hollow cylindrical forgings which were welded together. Alloy steel...