Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001817
EISBN: 978-1-62708-241-9
... ultimately caused the rope to fail. wire rope ductile fracture undersized sheave extra improved plow steel cup and cone fracture profile dimples fractographic analysis sheave pitch to rope diameter ratio 1096 (extra improved plow steel, high carbon steel) Introduction Physical Study...