Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.matlhand.c0048068
EISBN: 978-1-62708-224-2
... examination and the metal was showed by chemical analysis to be semikilled 1015 steel. The fatigue fracture was concluded to have initiated in the intergranular oxidation region and the failure of the hook was contributed by the poor fatigue and impact properties of the forged structure. As a corrective...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.matlhand.c0048068
EISBN: 978-1-62708-224-2
... examination and the metal was showed by chemical analysis to be semikilled 1015 steel. The fatigue fracture was concluded to have initiated in the intergranular oxidation region and the failure of the hook was contributed by the poor fatigue and impact properties of the forged structure. As a corrective...
Series: ASM Failure Analysis Case Histories
Volume: 2
Publisher: ASM International
Published: 01 December 1993
DOI: 10.31399/asm.fach.v02.c9001286
EISBN: 978-1-62708-215-0
...Abstract Abstract Failure of AISI 1015 steel brake discs used in power transmissions in emergency winches was investigated using various testing methods. The failed discs were stampings that had replaced cast discs. Residual stresses in the fillets of new cast and new stamped brake discs were...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001759
EISBN: 978-1-62708-241-9
... for Carbonitrided and Hardened Samples The bearing cup tested by push-out load test bearing cup was found to withstand push-out load of 885 kg. Push-Out Load Test Results for Nitrided Samples The bearing cup tested by push-out load test and was found to withstand push-out load of 1015 kg. To check...
Series: ASM Failure Analysis Case Histories
Volume: 1
Publisher: ASM International
Published: 01 December 1992
DOI: 10.31399/asm.fach.v01.c9001073
EISBN: 978-1-62708-214-3
... in the hot-rolled, normalized, and annealed conditions Table 1 Hardness properties of selected carbon steels in the hot-rolled, normalized, and annealed conditions AISI grade Condition or treatment Hardness, HB 1015 As-rolled 126 Normalized at 925 °C (1700 °F) 121 Annealed at 870 °C...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.auto.c0001784
EISBN: 978-1-62708-218-1
... 302–321 980 142 825 120 440 64 350 51 220 32 160 23 321–352 1040 151 895 130 470 68 365 53 225 33 160 23 352–375 1145 166 1015 147 510 74 395 57 235 34 165 24 375–401 1215 176 1090 158 535 78 405 59 240 35 170 25 401–429 1295 188 1180 171...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.chem.c9001738
EISBN: 978-1-62708-220-4
.... This was done to create a test situation as close as possible to the real situation. The material taken from the manifold had undergone a diametrical expansion of 1.75% during service. A stress of 12 MPa was chosen, which is 20% higher than the hoop stress. Temperatures of 900 to 1015°C were used during...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0001811
EISBN: 978-1-62708-180-1
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003563
EISBN: 978-1-62708-180-1
.... Thermal Spray Conf. , (Singapore), ASM International , 2001 , p 1009 – 1015 83. Tobe S. , Kodama S. , and Misawa H. , Rolling Fatigue Behaviour of Plasma Sprayed Coatings on Aluminum Alloy , Proc. Nat. Thermal Spray Conf. 1990 ( Tokyo, Japan ), ASM International , 1990 , p...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003510
EISBN: 978-1-62708-180-1
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006829
EISBN: 978-1-62708-295-2
... , p 1005 – 1015 10.1016/j.triboint.2006.02.038 152. Godfrey D. and Bisson E.E. , “ Bonding of Molybdenum Disulphide to Various Materials to Form a Solid Lubricating Film, Part II: Friction and Endurance Characteristics of Films Bonded by Practical Methods ,” Technical Note 2802...