1-20 of 26 Search Results for

100% Nb

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.homegoods.c9001610
EISBN: 978-1-62708-222-8
... variable of the material that may promote adverse reactions. Body piercing ISO 5832-1 Fe-17Cr-8Ni Fe-16Cr-8Ni-2.3Mo Fe-17Cr-10Ni-2.4Mo 100% Nb Pitting corrosion (Other, miscellaneous, or unspecified) failure Surface treatment related failures The body piercing of the upper portions...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001816
EISBN: 978-1-62708-241-9
.... structural components superplastic deformation boundary sliding dislocation creep high-strength low alloy steel decohesions traction testing grain size elongation Ti-Nb microalloyed ultrafine-grained steel (UGS steel, general) high-strength low-alloy steel (HSLA steel, general) Introduction...
Series: ASM Failure Analysis Case Histories
Volume: 1
Publisher: ASM International
Published: 01 December 1992
DOI: 10.31399/asm.fach.v01.c9001046
EISBN: 978-1-62708-214-3
... of the same alloys, along with Inconel alloys 601, 617, and 690 and stainless steel type 347 was also conducted in a simulated waste incinerator nitrogen atmosphere containing 10% Co2, 9% O2, 4% HCl, 130 ppm HBr and 100 ppm SO2 at 595, 705, 815, and 925 deg C (1100, 1300,1500, and 1700 deg F). The tests...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.med.c9001690
EISBN: 978-1-62708-226-6
... implants. Corrosion Fracture mechanisms Metallic surgical implants Retrieval analysis Ti-6Al-4V UNS R56406 316L UNS S31603 ISO 5832-2 grade 1 Nitinol (Other, general, or unspecified) corrosion (Other, general, or unspecified) fracture Worldwide data indicate that approximately 100...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.conag.c9001723
EISBN: 978-1-62708-221-1
... rolled from a rimming steel ingot. Fig. 9 Showing section through sheared end of tie-bar ×50 Fig. 10 Section adjacent to fractured edge ×100 Fig. 11 Sulphur print indicating that the tie-bar was made From rimming steel The following tests, unless otherwise stated, were...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001803
EISBN: 978-1-62708-241-9
... be broken down into several categories: misuse; assembly or implantation errors; design errors, including improper selection of materials; corrosion; corrosion fatigue; and wear. According to statistical data, approximately 100 million metallic implants were installed in humans between 1940 and 1975...
Series: ASM Failure Analysis Case Histories
Volume: 2
Publisher: ASM International
Published: 01 December 1993
DOI: 10.31399/asm.fach.v02.c9001341
EISBN: 978-1-62708-215-0
...Abstract Abstract An SB407 alloy 800H tube failed at a 100 deg bend shortly after startup of a new steam superheater. Three bends failed and one bend remote from the failure area was examined. Visual examination showed that the fracture started on the outside surface along the inside radius...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.modes.c0047010
EISBN: 978-1-62708-234-1
... 0.10 18.2 53.0 3.1 18.0 1.1 Ti, 5.4 Nb+Ta, 0.5 Al H19 tool steel 0.40 0.29 0.23 4.1 0.44 86.0 4.1 Co, 4.0 W, 2.1 V Udimet 630 0.03 0.15 0.10 17.3 57.0 2.9 17.5 1.0 Ti, 0.10 Co, 0.6 Al René 41 0.09 0.04 0.10 18.8 55.0 9.8 1.4 3.2 Ti, 11.3 Co, 1.6 Al Heat...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.chem.c9001738
EISBN: 978-1-62708-220-4
... (typically made of HK40 or HP40+Nb) and flows down through each tube and is collected in a bottom manifold. The partially reformed gases contain hydrogen, carbon monoxide, carbon dioxide, methane and steam. Then the gases flow towards the riser (typically made of HP40+Nb or Supertherm), and from...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001840
EISBN: 978-1-62708-241-9
..., Inconel 625 plate with dimensions of 150 × 100 × 3 mm was clad on ASTM A517 low carbon steel plate with dimensions of 130 × 80 × 20 mm. The chemical composition of materials measured by quantometer is listed in Table 1 . Also, both plates were chosen in annealed condition to avoid the likely effect...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001768
EISBN: 978-1-62708-241-9
... to assess the chemical composition using the standard method. The chemical composition of the cracked plate vis-à-vis the standard is provided in Table 1 . Chemistry of the cracked splice plate Table 1 Chemistry of the cracked splice plate Sample type C Si Mn P S Al V Nb Splice...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.bldgs.c9001171
EISBN: 978-1-62708-219-8
... . 5. Rogers T. H. , Marine Corrosion, G. Newnes , London ( 1968 ) 81 . 6. Kauczor E. , Der Praktiker 1 ( 1972 ) 9 . 7. Wilson F. G. , Br. Corros. J. 6 ( 1971 ) 100 . 10.1179/000705971798323874 8. Joshi A. , Stein D. F. , Corrosion NACE 28...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.bldgs.c9001135
EISBN: 978-1-62708-219-8
... , ASM , 1985 . 5. Tobler R.L. , and Cheng Y.W. , “Midrange Fatigue Crack Growth Data Calculations for Structural Alloys at Room and Cryogenic Temperatures,” NBS, Boulder Co. , Unpublished. Selected References Selected References • Fisher J.W. , Failures of Bridge...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.modes.c9001712
EISBN: 978-1-62708-234-1
... composition of UCX not provided due to proprietary nature. Fe balance for all alloys. Table 4 Chemical analysis of the alloys used in the experiment. Complete composition of UCX not provided due to proprietary nature. Fe balance for all alloys. Alloy C Si Mn Cr Ni Mo Nb W Co Ti N...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.conag.c9001637
EISBN: 978-1-62708-221-1
... (Emission Spectroscopy) Table 1 Bolt Compositions (Emission Spectroscopy) Bolt Bolt Comp %C %Mn %Si %Ni %Cr %Mo %S %P %Cu %Nb %V %Ti %Al %B ID Type Type 1 HPC (a) C1 0.41 1.83 0.21 0.01 0.02 <0.01 0.120 0.026 0.01 0.01 0.12 0.01 0.01 0.003 2 HPC...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001828
EISBN: 978-1-62708-241-9
... III sub-section NB and to quality assurance requirements of the Canadian Standards Association (CSA) Code Z 299.1 (equivalent to ISO 9001). The pump is coupled to the motor through a rigid spacertype coupling. Each pump is driven by a three-phase vertical induction motor. The nameplate rating...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0001822
EISBN: 978-1-62708-180-1
...Chemical analysis of axles 1611 and 2028<xref rid="n0010069" ref-type="table-fn">(a)</xref> Table 1 Chemical analysis of axles 1611 and 2028 (a) Axle Element, % C (b) Mn (c) P (d) S (b) Si (e) Ni (f) Cr (f) Mo (f) Al (a) Sn (g) Cu (h) V (f) Nb (g) Ti (g) N...
Book Chapter

Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003562
EISBN: 978-1-62708-180-1
... of material per unit of sliding distance per unit of applied normal load), the curves are of the form shown in Fig. 13 . The curves are sigmoidal, with the specific wear rate becoming constant at amplitudes &gt;100 μm (&gt;0.004 in.) (that is, identical with unidirectional sliding or reciprocating sliding...
Book Chapter

Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003548
EISBN: 978-1-62708-180-1
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003552
EISBN: 978-1-62708-180-1
... high-velocity conditions where the protective film erodes away as rapidly as it forms. Hydrogen contents of 100 to 200 ppm may cause severe losses in tensile ductility and notched tensile strength in titanium alloys and may cause brittle delayed failure under sustained loading conditions...