Skip Nav Destination
Close Modal
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-5 of 5
Nickel-iron alloys
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.petrol.c9001638
EISBN: 978-1-62708-228-0
Abstract
An Incoloy 800H (UNS N08810) transfer line on the outlet of an ethane-cracking furnace failed during decoking of the furnace tubes after nine years in service. A metallographic examination using optical and scanning electron microscopy as well as energy-dispersive x-ray spectroscopy revealed that the failure was due to sulfidation. The source of the sulfur in the furnace effluent was either dimethyl disulfide, injected into the furnace feed to prevent coke formation and carburization of the furnace tubes, or contamination of the feed with sulfur bearing oil.
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.marine.c9001164
EISBN: 978-1-62708-227-3
Abstract
Plate perforation occurred in the cylindrical section and walls of the inlet foot (2.38 mm thick Incoloy 825 plate welded using INCO welding rod 135) of an inert gas fire prevention system in an oil tanker. Cross-sectional microprobe analysis showed the corrosion product to contain sulfur, mainly from the flue gas, and calcium and chlorine, mainly from the sea water. The gray corrosion product was interspersed with rust and a black carbonaceous deposit. Corrosion pitting and poor weld penetration, with carbide precipitation and heavy etching at grain boundaries, indicated sensitization and susceptibility to aqueous intergranular corrosion. Chemical analysis showed the predominant acid radical to be sulfate (6.20% in the carbonaceous deposit and 0.60% in the corrosion product), suggesting that oxidation of SO2 in the flue gas caused the corrosion. Moisture condensation, the carbon acting as a cathode, and alloy susceptibility to intergranular corrosion contributed to the corrosion.
Book Chapter
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.process.c0049796
EISBN: 978-1-62708-235-8
Abstract
Problems with materials compatibility were encountered in pyrotechnically driven devices used in a number of ordnance applications requiring rapid mechanical actuation. A fine bridgewire is located in contact with the chemical pyrotechnic, and the charge is ignited by electrical heating of the bridgewire. Evidence of severe corrosion was revealed on examination of the nickel-chromium-iron alloy bridgewire and the nickel-iron alloy pins. Metallic elements in the pin or bridgewire and substantial amounts of chlorine were detected from the x-ray spectra. Morphological changes indicative of decomposition and dissolution were revealed to have occurred in regions of the pyrotechnic that had been in contact with the bridgewire and pin surfaces by examination of the titanium-potassium perchlorate (Ti-K-Cl-O4) pyrotechnic. Substantial amounts of water were revealed to be associated with the surfaces of the titanium particles in the pyrotechnic by nuclear magnetic resonance. It was proposed that the chlorine-containing residue combined with the water from the pyrotechnic to form a thin aqueous film corroding the bridgewire and pins. A new cleaning procedure was implemented for the glass headers to eliminate the chloride contamination and a vacuum drying procedure was instituted for the pyrotechnic.
Series: ASM Failure Analysis Case Histories
Volume: 1
Publisher: ASM International
Published: 01 December 1992
DOI: 10.31399/asm.fach.v01.c9001105
EISBN: 978-1-62708-214-3
Abstract
A tie rod, nut, and bellows from a failed 610 mm (24 in.) diam tied universal expansion joint that carried tail gases consisting of N 2 + O 2 with slight traces of nitrogen oxides and water were examined. The materials were SA 193-B7 (AISI 4140), SA 194–214, and Incoloy 800H, respectively. Visual examination of the bellows revealed cracks in heavily cold-worked areas (both inside and outside) and considerable corrosion. SEM analysis showed a classical intergranular failure pattern with microcracking. The threaded tie rod microstructure contained spheroidized carbide that was more pronounced at the tie rod end of the failure. Energy-dispersive X-ray analysis of fracture surfaces from the bellows showed the presence of chlorine and sulfur. Failure of the bellows was attributed to stress-corrosion cracking, with chlorine and sulfur being the corroding agents. The rod damage was the result of failure of the bellows, which allowed escaping hot gases to impinge on the tie rods and heat them to approximately 595 deg C (1100 deg F). It was recommended that the insulation be analyzed to determine the origin of the chlorine and sulfur and that it be replaced if necessary.
Series: ASM Failure Analysis Case Histories
Volume: 1
Publisher: ASM International
Published: 01 December 1992
DOI: 10.31399/asm.fach.v01.c9001108
EISBN: 978-1-62708-214-3
Abstract
The curved parts of exit pigtails made of wrought Incoloy 800H tubing used in steam reforming furnaces failed by performance after a period of service shorter than that predicted by the designers. Examination of a set of tubes consisting of both curved (perforated) and straight parts revealed that the cracks initiated at the outer surface by a combined mechanism of creep and intergranular embrittlement. A smaller grain size resulting from cold bending fabrication procedures for the curved parts was responsible for accelerating the embrittlement. It was recommended that hot bending be used for fabrication of the curved parts. A change of alloy to a low-alloy chromium-molybdenum allay to protect against heat was also suggested.