Practical Heat Treating (Second Edition)
Appendix D: Use of Test Coupons for Process Verification
-
Published:2006
Abstract
The results of certain heat treating processes must be verified for case quality and case depth by destructively sectioning a part or parts that were subjected to the process. Test coupons or test pins are often used for diffusion processes such as carburizing, carbonitriding, nitriding, and ferritic nitrocarburizing to provide an accurate heat treating process evaluation. This appendix briefly describes the advantages and selection and design considerations of test coupons. A typical example of the use of test pins for monitoring carburizing and hardening of gears is provided.
Use of Test Coupons for Process Verification, Practical Heat Treating, 2nd ed., By Jon L. Dossett, Howard E. Boyer, ASM International, 2006, p 283–286, https://doi.org/10.31399/asm.tb.pht2.t51440283
Download citation file:
New Handbook: Volume 11B
Now available in the Digital Library! Volume 11B serves as a reference and guide to help engineers determine the causes of failure in plastic components and make corrective adjustments through design and manufacturing modifications.