Appendix B: Decarburization of Steels
-
Published:2006
Abstract
This appendix discusses in brief the sources of decarburization of steels as well as the effect of heat treatment on the process.
You do not currently have access to this chapter.
Citation
Decarburization of Steels, Practical Heat Treating, 2nd ed., By Jon L. Dossett, Howard E. Boyer, ASM International, 2006, p 275–278, https://doi.org/10.31399/asm.tb.pht2.t51440275
Download citation file:
New Handbook: Volume 11B
Volume 11B serves as a reference and guide to help engineers determine the causes of failure in plastic components and make corrective adjustments through design and manufacturing modifications.
Related Book Content
Alteration of Microstructure
Metallographer’s Guide Practices and Procedures for Irons and Steels
Heat Treatment Problems Associated with Design and Steel Selection
Heat Treating of Irons and Steels
Introduction
Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels
Failures from the Casting Process
Failure Analysis of Heat Treated Steel Components
Steel Decarburization—Mechanisms, Models, Prevention, Correction, and Effects on Component Life
Steel Heat Treating Technologies
Metallurgical Investigation of Failed Locked Coil Track Ropes Used in a Mining Conveyor
Handbook of Case Histories in Failure Analysis
Heat Treatment of Gears
Heat Treatment of Gears A Practical Guide for Engineers
Decarburization and Defects
Practical Induction Heat Treating (Second Edition)
Austenitizing and Typical Heat Treatment Temperatures for Steels
Heat Treating of Irons and Steels
Origin of Microstructure
Metallographer’s Guide Practices and Procedures for Irons and Steels