Book Chapter
Chapter 1: What Is Heat Treating? Importance and Classifications
-
Published:2006
Abstract
This chapter introduces the principal heat treating processes, namely normalizing, annealing, stress relieving, surface hardening, quenching, and tempering. An overview of four of the more popular surface hardening treatments, namely carburizing, carbonitriding, nitriding, and nitrocarburizing, is provided.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
What Is Heat Treating? Importance and Classifications, Practical Heat Treating, 2nd ed., By Jon L. Dossett, Howard E. Boyer, ASM International, 2006, p 1–7, https://doi.org/10.31399/asm.tb.pht2.t51440001
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field
Related Book Content
Heat Treating of Mold Steels and Corrosion-Resistant Tool Steels
Heat Treating of Irons and Steels
Conventional Heat Treatment—Basic Concepts
Metallography of Steels Interpretation of Structure and the Effects of Processing
Use of Test Coupons for Process Verification
Practical Heat Treating (Second Edition)
Heat Treating of High-Speed Tool Steels
Heat Treating of Irons and Steels
Introduction to Heat Treating of Tool Steels
Heat Treating of Irons and Steels
Case Hardening of Steel
Practical Heat Treating (Second Edition)
Surface Hardening
Steels: Processing, Structure, and Performance (Second Edition)
Heat Treatment of Steel
Elements of Metallurgy and Engineering Alloys
Mold Steels
Tool Steels (Fifth Edition)
Through-Hardening Gears
Heat Treatment of Gears A Practical Guide for Engineers