Abstract
Fracture mechanics is a well-developed quantitative approach to the study of failures. This chapter discusses fracture toughness and fracture mechanics, linear-elastic fracture mechanics, and modes of loading. The discussion also covers plane strain and stress and crack growth kinetics. The chapter presents a case history that illustrates the use of fracture mechanics in failure analysis. An appendix provides a more detailed discussion of fracture mechanics concepts.
You do not currently have access to this chapter.
Citation
Fracture Mechanics, Understanding How Components Fail, 3rd ed., By Donald J. Wulpi;Edited By Brett Miller, ASM International, 2013, p 257–279, https://doi.org/10.31399/asm.tb.uhcf3.t53630257
Download citation file:
Related Book Content
Engineering Aspects of Failure and Failure Analysis
Metals Handbook Desk Edition (2nd Edition)
Fracture Toughness of Ceramics and Ceramic Matrix Composites
Mechanical Testing and Evaluation
Fracture Toughness and Fracture Mechanics
Mechanical Testing and Evaluation
Plastic Deformation: Strain and Strain Rate
Cold and Hot Forging Fundamentals and Applications
Fracture Resistance of Structural Alloys
Fatigue and Fracture
Fatigue and Fracture Mechanics
Mechanical Testing and Evaluation
Fracture Mechanics in Failure Analysis
Fatigue and Fracture
Brittle Fracture in a Large Grain Storage Bin
Handbook of Case Histories in Failure Analysis
Stress Analysis and Fracture Mechanics
Failure Analysis and Prevention