Book Chapter
Chapter 3: Systems and Systems Failure Analysis Concepts
-
Published:2009
Abstract
A system failure occurs when a system does not do what it is supposed to do when it is supposed to do it, or it does something it is not supposed to do. This chapter provides a basic understanding of how failures occur, how systems operate, and the types of failures, namely intermittent and inadvertent system failures.
You do not currently have access to this chapter.
Citation
Systems and Systems Failure Analysis Concepts, Systems Failure Analysis, By Joseph Berk, ASM International, 2009, p 19–24, https://doi.org/10.31399/asm.tb.sfa.t52780019
Download citation file:
New Handbook: Volume 11B
Volume 11B serves as a reference and guide to help engineers determine the causes of failure in plastic components and make corrective adjustments through design and manufacturing modifications.
Related Book Content
Failure Analysis Terms and Definitions
Microelectronics Failure Analysis: Desk Reference (Seventh Edition)
The Failure Analysis Process: An Overview
Failure Analysis and Prevention
Failure Analysis: Why and for Whom?
Failure Analysis of Engineering Structures Methodology and Case Histories
Failure Analysis and After
Failure Analysis of Engineering Structures Methodology and Case Histories
Glossary of Terms—Failure Analysis and Prevention
Failure Analysis and Prevention (2021 Edition)
Component Failure Causes and Suggested Analysis Methods
Systems Failure Analysis
Techniques of Failure Analysis
Understanding How Components Fail (Third Edition)
Failure Analysis Methodology
Failure Analysis of Engineering Structures Methodology and Case Histories
Glossary of Terms—Characterization and Failure Analysis of Plastics
Characterization and Failure Analysis of Plastics
Abbreviations—Characterization and Failure Analysis of Plastics
Characterization and Failure Analysis of Plastics