Chapter 7: Diffusion—A Mechanism for Atom Migration within a Metal
-
Published:2007
Abstract
Diffusion is the primary mechanism by which carbon atoms move or migrate in iron. It is driven by concentration gradients and aided by heat. This chapter provides a practical understanding of the diffusion process and its role in the production and treatment of steel. It discusses the factors that determine diffusion rates and distances, including time, temperature, and the relative size of the atoms involved. It also describes two heat treating methods, carburizing and decarburizing, where carbon diffusion plays a central role.
Sign in
ASM members
Member Sign InDiffusion—A Mechanism for Atom Migration within a Metal, Steel Metallurgy for the Non-Metallurgist, By John D. Verhoeven, ASM International, 2007, p 63–70, https://doi.org/10.31399/asm.tb.smnm.t52140063
Download citation file:
March 14-16 | Fort Worth, Texas
Keep up to date with the latest aerospace materials and technologies. Register today for Aeromat 2023!